MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Ascend Performance Materials Starflam® AFR470X2 PA66-GF35 FR
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Glass Fiber Filled, Flame Retardant

Material Notes: Starflam AFR470X2 is a glass filled, red phosphorous flame retardant PA66 for injection molded applications.

Information provided by Ascend Performance Materials.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.44 g/ccDAM; ISO 1183
Water Absorption 1.6 %
@Temperature 23.0 °C,
Time 86400 sec
DAM; ISO 62
Moisture Absorption at Equilibrium 1.4 %
@Temperature 23.0 °C
DAM; ISO 62
Water Absorption at Saturation 4.5 %
@Temperature 23.0 °C
ISO 62
Linear Mold Shrinkage, Flow 0.0030 cm/cm
@Thickness 2.00 mm
DAM; ISO 294-4
Linear Mold Shrinkage, Transverse 0.0090 cm/cm
@Thickness 2.00 mm
DAM; ISO 294-4
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 105 MPa50% RH; ISO 527-2
 155 MPaDAM; ISO 527-2
Elongation at Break 2.4 %DAM; ISO 527-2
 3.9 %50% RH; ISO 527-2
Tensile Modulus 7800 MPa50% RH; ISO 527-2
 11000 MPaDAM; ISO 527-2
Flexural Strength 155 MPa50% RH; ISO 178
 218 MPaDAM; ISO 178
Flexural Modulus 7500 MPa50% RH; ISO 178
 10600 MPaDAM; ISO 178
Poissons Ratio 0.34ISO 527-2
Izod Impact, Notched (ISO) 7.70 kJ/m²
@Temperature -40.0 °C
DAM; ISO 180/1A
 7.80 kJ/m²
@Temperature -30.0 °C
DAM; ISO 180/1A
 9.00 kJ/m²
@Temperature -40.0 °C
50% RH; ISO 180/1A
 9.20 kJ/m²
@Temperature -30.0 °C
50% RH; ISO 180/1A
 11.0 kJ/m²
@Temperature 23.0 °C
DAM; ISO 180/1A
 14.0 kJ/m²
@Temperature 23.0 °C
50% RH; ISO 180/1A
Charpy Impact Unnotched 55.0 kJ/m²
@Temperature -40.0 °C
50% RH; ISO 179/1eU
 58.0 kJ/m²
@Temperature -30.0 °C
50% RH; ISO 179/1eU
 58.0 kJ/m²
@Temperature -40.0 °C
DAM; ISO 179/1eU
 59.0 kJ/m²
@Temperature -30.0 °C
DAM; ISO 179/1eU
 71.0 kJ/m²
@Temperature 23.0 °C
DAM; ISO 179/1eU
 75.0 kJ/m²
@Temperature 23.0 °C
50% RH; ISO 179/1eU
Charpy Impact, Notched 8.90 kJ/m²
@Temperature -40.0 °C
50% RH; ISO 179/1eA
 9.30 kJ/m²
@Temperature -30.0 °C
50% RH; ISO 179/1eA
 10.0 kJ/m²
@Temperature -30.0 °C
DAM; ISO 179/1eA
 10.0 kJ/m²
@Temperature -40.0 °C
DAM; ISO 179/1eA
 12.0 kJ/m²
@Temperature 23.0 °C
DAM; ISO 179/1eA
 15.0 kJ/m²
@Temperature 23.0 °C
50% RH; ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+15 ohm-cm
@Thickness 1.00 mm
DAM; IEC 60093
Dielectric Strength 25.0 kV/mm
@Thickness 1.00 mm
50% RH; IEC 60243
 27.0 kV/mm
@Thickness 1.00 mm
DAM; IEC 60243
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 19.0 µm/m-°C
@Thickness 2.00 mm,
Temperature 23.0 - 55.0 °C
DAM; ISO 11359-2
CTE, linear, Transverse to Flow 100 µm/m-°C
@Thickness 2.00 mm,
Temperature 23.0 - 55.0 °C
DAM; ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 255 °CUnannealed; 50% RH; ISO 75-2/B
 256 °CUnannealed; DAM; ISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi) 182 °CUnannealed; 50% RH; ISO 75-2/A
 237 °CUnannealed; DAM; ISO 75-2/A
UL RTI, Electrical 100 °C
@Thickness 0.750 mm
UL 746
 100 °C
@Thickness 3.00 mm
UL 746
UL RTI, Mechanical with Impact 95.0 °C
@Thickness 0.750 mm
UL 746
 100 °C
@Thickness 3.00 mm
UL 746
UL RTI, Mechanical without Impact 100 °C
@Thickness 0.750 mm
UL 746
 105 °C
@Thickness 3.00 mm
UL 746
Flammability, UL94 V-0
@Thickness 0.750 mm
UL 94
 V-0
@Thickness 3.00 mm
UL 94
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature >= 275 °CInjection
 <= 285 °CInjection
Middle Barrel Temperature >= 275 °CInjection
 <= 285 °CInjection
Front Barrel Temperature >= 275 °CInjection
 <= 285 °CInjection
Melt Temperature >= 275 °CInjection
 <= 285 °CInjection
Mold Temperature >= 70.0 °CInjection
 <= 90.0 °CInjection
Drying Temperature >= 75.0 °CInjection
 <= 85.0 °CInjection
Dry Time 4.00 hourInjection
Moisture Content 0.10 %Injection
 
Descriptive Properties
AdditiveFlame Retarding Agent
 Heat Stabilizer
 Release agent
AppearanceNatural Color
FeaturesFlame Retardant
 Halogen Content, None
FormsPellets
Processing MethodInjection Molding
RegionNorth America, Europe

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PASCE9116 / 287567

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.