MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Matexcel CER-0056 Mica sheets (Muscovite or Phlogopite)
Categories: Ceramic; Oxide; Silicon Oxide

Material Notes: Our mica sheets are the ideal alternative for asbestos insulations. Good resistance to high temperatures & chemicals, low heat conductivity, high dielectric strength, good high-voltage proof performance. Fire resistance classification UL94 (94 V-0), BS 479 (class 1), NBN 21-203 (A1).

Mica sheets (Muscovite or Phlogopite)

Application: Used for high-performance thermal and electrical insulation in a broad range of industries such as: heating elements for electrical & thermo mechanical equipment construction of induction, arc or high frequency furnaces high voltage applications high thermal applications industrial sealing & gasket industries (e.g. oil & gas distribution)

Key Words: Synonyms: Mica sheets (Muscovite or Phlogopite)
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Particle Size 100 - 101600 µm
 
Descriptive Properties
ComponentsMica sheets consist of 85–90% high-grade Muscovite alternatively Phlogopite mica paper impregnated with an outstanding high temperature resistant silicone resin.
Purity85–90%

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PMXCK1493 / 300124

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.