Typical uses include machine, plow, and carriage bolts, tie wire, cylinder head studs, and machined parts, U-bolts, concrete reinforcing rods, forgings, and non-critical springs. Post oil quenched hardness: 50 HRC surface, 97 HRB half-radius, 95 HRB center. |
UNS G10400, ASTM A29, ASTM A108, ASTM A510, ASTM A519, ASTM A546, ASTM A576, ASTM A682, MIL SPEC MIL-S-11310 (CS1040), SAE J403, SAE J412, SAE J414, DIN 1.1186, JIS S 40 C, BS 970 060A40, BS 970 080A40, BS 970 080M40 (EN8), BS 2 S 93 |