MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Lucas-Milhaupt EASY FLO 45 Silver Based Cadmium-Bearing Filler Metal
Categories: Metal; Nonferrous Metal; Precious Metal; Silver Alloy; Solder/Braze Alloy

Material Notes: Easy-Flo 45 is very versatile and can be used successfully on nearly all nickel, iron and copper base alloys. In certain instances, special fluxes, may be required to obtain good wetting and bonding. In brazing gray cast iron it is necessary to treat the surface prior to brazing to remove graphite, in order to assure good wetting by the brazing filler metal.

A complete list of the uses of Easy-Flo 45 would include practically all applications for which silver brazing filler metals have been used.

Characteristics: Easy-Flo 45 is a eutectic type, free-flowing filler metals that, because of their narrow melting range, are less sensitive to the rate of heating and should not liquate (i.e. separate into low and high melting constituents). This high fluidity makes well-fitted joints essential and prevents bridging or large fillet formation. Handy Flux should be used with either of these filler metals.

Some base metals when brazed under high stress may crack during brazing when the stressed base metal is wetted by the brazing filler metal. This is a form of stress corrosion cracking. The low flow temperature of Easy-Flo is below the stress relaxation temperature of some nickel base alloys. The cure is to relieve the stress before the brazing alloy is applied. A higher melting brazing filler metal may be preferred since stress relief will then occur before the filler metal melts.

Specifications:This filler metal conform to the following specifications: AWS A5.8 BAg-1, SAE-AMS 4769, ASME Boiler and Pressure Vessel Code Section II-C SFA 5.8 BAg-1

Information provided by Lucas-Milhaupt, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 9.42 g/cc
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 55000 psiArmco Iron (0.05% C) butt joint
 60000 psiStainless Steel (18-8) Annealed butt joint
 65000 psi1020 Steel butt joint
 85000 psi1095 (Drill Rod) butt joint
 90000 psiHigh Speed Steel (18 W, 4 Cr, 1 V) butt joint
 110000 psi4140 Steel butt joint
 130000 psiStainless Steel 918-8) Cold Rolled butt joint
 45000 psi
@Temperature 23.0 °C
 70000 psi
@Temperature 23.0 °C
 101000 psi
@Temperature 23.0 °C
Tensile Strength, Ultimate 8000 psi
@Temperature 482 °C
Inconel butt joint
 12000 psi
@Temperature 427 °C
Stainless Steel (18-8) butt joint
 13000 psi
@Temperature 482 °C
Monel butt joint
 38000 psi
@Temperature 260 °C
Inconel butt joint
 48000 psi
@Temperature 260 °C
Monel butt joint
 49000 psi
@Temperature 260 °C
Stainless Steel (18-8) butt joint
Elongation at Break 0.00 %
@Temperature 260 °C
in 2", Stainless Steel (18-8) butt joint
 0.00 %
@Temperature 260 °C
in 2", Inconel butt joint
 0.00 %
@Temperature 427 °C
in 2", Stainless Steel (18-8) butt joint
 0.00 %
@Temperature 482 °C
in 2", Inconel butt joint
 0.00 %
@Temperature 482 °C
in 2", Monel butt joint
 0.00 %
@Temperature 23.0 °C
 0.00 %
@Temperature 23.0 °C
 3.1 %
@Temperature 260 °C
in 2", Monel butt joint
 7.3 %
@Temperature 23.0 °C
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00000606 ohm-cm
 
Thermal PropertiesOriginal ValueComments
Melting Point 1125 - 1145 °F
Solidus 1125 °FMelting Point
Liquidus 1145 °FFlow Point
 
Processing PropertiesOriginal ValueComments
Processing Temperature 1145 - 1350 °FBrazing Range
 
Component Elements PropertiesOriginal ValueComments
Cadmium, Cd 23 - 25 %
Copper, Cu 14 - 16 %
Other, total <= 0.15 %
Silver, Ag 44 - 46 %
Zinc, Zn 14 - 18 %
 
Descriptive Properties
ColorLight Yellow

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Lucas-Milhaupt Cerametil 616 Active Metal Brazing
Lucas-Milhaupt EASY FLO Silver Based Cadmium-Bearing Filler Metal
Indium Corp. Indalloy 215 Silver Solder Alloy
Lucas-Milhaupt Cerametil 716 Active Metal Brazing
Lucas-Milhaupt Lithobraze 925 Silver Based Cadmium Free Filler Metal

NLUCMI44 / 18111

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.