MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
3M Scotchcast™ 263 Electrical Epoxy Powder Resin
Categories: Polymer; Thermoset; Epoxy; Epoxy Cure Resin

Material Notes: 3M Scotchcast Electrical Resin 263 is a widely used, well-known general purpose epoxy powder resin. A one part, green pigmented, rapid heat-curing product, it is designed to provide a continuous, tough moisture and chemical resistant dialectic coating to a variety of substrates. It is intended for use where high temperature cut-through resistant is required. Scotchcast Electrical Resin 263 is manufactured by a fusion blend process, ensuring that each individual particle of powder contains all the components necessary to effect a complete cure and attain stated performance properties. Scotchcast 263 is applied to an object that has been heated to a temperature above the melting point of the resin. On contact with the preheated application surface, the resin melts, flows to a controlled extent, then cures, bonding to the substrate and coalescing into a smooth, continuous, essentially uniform thick coating. It effectively coats flat surfaces and corners, as well as, high point. Uses for Scotchcast 263 include moisture proofing and insulating armatures, stators, buss bars and toroid cores.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.47 g/cccured; ASTM D794
 
Mechanical PropertiesOriginal ValueComments
Gardner Impact 100 in-lb12-15 mil coating 1/8" sandblasted steel panel Gardner 5/8: Radius Impact Tester
Abrasion 0.60[g] Removed from 12-15 mil coating; ASMT D4060
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength 1000 kV/in12 to 15 mil coating; ASTM D149
 
Processing PropertiesOriginal ValueComments
Cure Time 0.333 min
@Temperature 232 °C
 0.500 min
@Temperature 204 °C
 10.0 min
@Temperature 177 °C
 30.0 min
@Temperature 149 °C
Gel Time 0.116666 - Error in fixSigDigits: @digits must be between 1 and 12. @digits is: 15 min
@Temperature 193 °C
hot plate
Shelf Life 24.0 Month
@Temperature <=27.0 °C
 
Descriptive Properties
AppearanceGreen

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Trelleborg Emerson & Cuming Stycast® XT-1169 Two-Component Epoxy High Service Temp Encapsulant
Resin Technology Group TIGA 142-EX Toughened Epoxy Adhesive
Overview of materials for Epoxy Molding Compound
Lord Adhesives Fusor® 380NS / 383NS Epoxy Adhesive
Lord Adhesives Circalok™ 6031 A/B Epoxy Encapsulant

PMM35362 / 170109

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.