MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Celanese Crastin® FR684NH1 NC010 PBT-GF25FR(40)
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled; Polybutylene Terephthalate (PBT), Glass Fiber Filled, Flame Retardant

Material Notes: 25% Glass Reinforced, Flame Retardant, Non-Halogenated, Polybutylene Terephthalate

Former DuPont product acquired by Celanese in 2022.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.52 g/ccISO 1183
Water Absorption 0.25 %
@Thickness 2.00 mm
DS; Sim. to ISO 62
Moisture Absorption 0.100 %
@Thickness 2.00 mm
DS; Sim. to ISO 62
Linear Mold Shrinkage, Flow 0.0050 cm/cmISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.012 cm/cmISO 294-4, 2577
Spiral Flow 28.0 cm
@Pressure 110 MPa
width/thickness = 2mm
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 95.0 MPaISO 527-1/-2
Elongation at Break 2.5 %ISO 527-1/-2
Tensile Modulus 9400 MPaISO 527-1/-2
Poissons Ratio 0.34
Charpy Impact Unnotched 43.0 kJ/m²
@Temperature 23.0 °C
ISO 179/1eU
 46.0 kJ/m²
@Temperature -30.0 °C
ISO 179/1eU
Charpy Impact, Notched 6.80 kJ/m²
@Temperature -30.0 °C
ISO 179/1eA
 7.50 kJ/m²
@Temperature 23.0 °C
ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+15 ohm-cmIEC 62631-3-1
Surface Resistance >= 1.00e+15 ohmIEC 62631-3-2
Dielectric Strength 42.0 kV/mmIEC 60243-1
Comparative Tracking Index 600 VIEC 60112
 >= 600 VPLC 0; UL 746A
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 20.0 µm/m-°C
@Temperature 55.0 - 160 °C
ISO 11359-1/-2
 23.0 µm/m-°C
@Temperature -40.0 - 23.0 °C
ISO 11359-1/-2
 29.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
ASTM E 831
CTE, linear, Transverse to Flow 66.0 µm/m-°C
@Temperature -40.0 - 23.0 °C
ISO 11359-1/-2
Melting Point 223 °C10°C/min; ISO 11357-1/-3
Hot Ball Pressure Test 220 °CIEC 60695-10-2
Deflection Temperature at 1.8 MPa (264 psi) 205 °CISO 75-1/-2
Glass Transition Temp, Tg 55.0 °C10°C/min; ISO 11357-1/-2
Flammability, UL94 V-0
@Thickness 0.750 mm
IEC 60695-11-10
 V-0
@Thickness 1.50 mm
IEC 60695-11-10
Oxygen Index 40 %ISO 4589-1/-2
Glow Wire Ignition Temperature 750 °C
@Thickness 0.400 mm
IEC 60695-2-12
 750 °C
@Thickness 0.750 mm
IEC 60695-2-13
 750 °C
@Thickness 1.00 mm
IEC 60695-2-13
 750 °C
@Thickness 1.50 mm
IEC 60695-2-13
 800 °C
@Thickness 3.00 mm
IEC 60695-2-13
Glow Wire Flammability Index 960 °C
@Thickness 0.400 mm
IEC 60695-2-12
 960 °C
@Thickness 0.750 mm
IEC 60695-2-12
 960 °C
@Thickness 1.00 mm
IEC 60695-2-12
 960 °C
@Thickness 1.50 mm
IEC 60695-2-12
 960 °C
@Thickness 3.00 mm
IEC 60695-2-12
 
Processing PropertiesOriginal ValueComments
Melt Temperature 250 °COptimum, Injection
 240 - 260 °CRange, Injection
Mold Temperature 80.0 °COptimum, Injection
 30.0 - 130 °CInjection
Ejection Temperature 170 °CInjection
Drying Temperature 120 °CInjection
Dry Time 2.00 - 4.00 hourInjection, Dehumidified Dryer
Moisture Content <= 0.040 %Injection
Hold Pressure >= 60.0 MPaInjection
 
Descriptive Properties
AdditivesFlame retardant
 Non-halogenated/Red phosphorous free flame retardant
Back pressureAs low as possible
Drying RecommendedyesInjection
Emission of organic compounds (µgC/g)39VDA 277
Part Marking Code>PBT-GF25FR(40)<ISO 11469
PolymerPBT-GF25 FR(40)
Processing Hold Pressure Time (s/mm)3Injection
Railway classificationR22DIN 53236
Railway classification ratingHL1EN 45545-2
Resin IdentificationPBT-GF25FR(40)ISO 1043

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PDSX5015p / 254323

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.