MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Unifrax CC-Max® 4 HP Substrate Support Mat
Categories: Ceramic

Material Notes: CC-Max 4 HP mat is produced when the proprietary fiber is converted into a flexible flet-like product. The material is thermally stable and engineered to maintain a controlled holding force on the substrate across a wide temperature range from ambient to 1250°C (inlet gas temperature).

CC-Max 4 HP may also be used in applications which challenge the temperature limits of traditional vermiculite-based mat systems, such as deisel osidation catalyst and particulate filters. In many applications, exhaust gas temperatures may not be high enough to activate the vermiculite and provide sufficient holding force for the substrate. The spring-like fiber matrix of CC-Max 4 HP provides constant pressure on the substrate at temperatures well below the expansion point of vermiculite systems. Similarly, as a result of the product's unique properties, CC-Max 4 HP maintains its resiliency and substrate support at elevated temperatures when intumescent systems begin to lose function.

Information Provided by Unifrax I LLC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Loss On Ignition >= 6.5 %
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield >= 0.100 MPa
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 0.130 W/m-K
@Temperature 650 °C
ASTM-C177
 
Descriptive Properties
Binder System (%)4-8
Fiberfrax® Fibers (%)92-96

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Röhm Plexiglas® XT Soundstop® Extruded Acrylic

CUNIF017 / 97789

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.