MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Go Yen Chemical Hexaphenoxycyclotriphosphazene;HPCTP;Phenoxycyclotriphosphazene;PCPZ Flame Retardant
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: CAS No. 1184-10-7

Hexaphenoxycyclotriphosphazene can be applied on epoxy, FCCL, LED, powder coating, embedding material, high molecular material. Hexaphenoxycyclotriphosphazene owns outstanding hydrolytic resistance, mechanical property, which can enhance the adding value of products and provide excellent fireproof effect.

Intro: GO YEN CHEMICAL INDUSTRIAL CO., LTD. (GYC Group) is the most innovative flame retardant manufacture in Taiwan, we own the strongest R&D team and abundant functional product line, our technical staff has been enhancing the technology and developing new types of fireproof material based on customers’ demanding. Hexaphenoxycyclotriphosphazene can be applied on epoxy, FCCL, LED, powder coating, embedding material, high molecular material. Hexaphenoxycyclotriphosphazene owns outstanding hydrolytic resistance, mechanical property, which can enhance the adding value of products and provide excellent fireproof effect.

Applications:

  • Can be used in electronic grade flame retardant for epoxy related products
  • Fireproof for LED embedding material application
  • EMC: Epoxy Molding Compound flame retard
  • EPOXY and SILICON
  • Electronic plate material/ flame retard grade CCL/ flame retard grade PCB
  • Powder coating
  • Embedding material
  • High molecular material
  • Versatile high value application

Information provided by Go Yen Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Volatiles <= 0.20 %
Molecular Weight 693.57 g/mol
Ash <= 0.10 %
 
Thermal PropertiesOriginal ValueComments
Melting Point 112 - 115 °C
 
Descriptive Properties
AppearanceWhite Crystalline Powder
Purity>99%

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PGOYEN161 / 266469

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.