MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Inno-Comp INNOPOL® CS 2-3120 BPLU 9H0017 20% Talc-Filled, UV Stabilized Polypropylene Block-Copolymer
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene with 20% Talc Filler

Material Notes: INNOPOL® CS 2-3120 BPLU 9H0017 is a 20% talc filled, UV stabilized compound based on polypropylene block-copolymer.

INNOPOL® CS 2-3120 BPLU 9H0017 is developed for producing injection molded automotive components.

All information provided by INNO-COMP.

Key Words: PP-B
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.05 g/cc
@Temperature 23.0 °C
ISO 1183
Linear Mold Shrinkage, Flow 0.010 cm/cmISO 294
Linear Mold Shrinkage, Transverse 0.0080 cm/cmISO 294
Melt Flow 13 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ISO 1133
Ash 20 %
@Temperature 600 °C
ISO 3451-1/A
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 28.0 MPa50 mm/min; ISO 527-1,-2
Elongation at Break 15 %ISO 527-1,-2
Elongation at Yield 3.5 %50 mm/min; ISO 527-1,-2
Tensile Modulus 2530 MPa1 mm/min; ISO 527-1,-2
Flexural Modulus 2740 MPa2 mm/min; ISO 178
Charpy Impact Unnotched 2.50 J/cm²
@Temperature -30.0 °C
ISO 179/1eU
 6.50 J/cm²
@Temperature 23.0 °C
ISO 179/1eU
Charpy Impact, Notched 0.150 J/cm²
@Temperature -30.0 °C
ISO 179/1eA
 0.400 J/cm²
@Temperature 23.0 °C
ISO 179/1eA
 
Thermal PropertiesOriginal ValueComments
Melting Point 165 °CDSC; ISO 11357-1,-3
Deflection Temperature at 0.46 MPa (66 psi) 125 °CISO 75-1,-2
Deflection Temperature at 1.8 MPa (264 psi) 62.0 °CISO 75-1,-2
Flammability, UL94 HB
@Thickness 1.60 mm
FMVSS 302
 
Descriptive Properties
Automotive MaterialsPassFMVSS 302
ColorBlack 9H0017

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Niche Polymer PPHT40BK Homopolymer PP, 40% Talc Fiber Filled
A. Schulman Lucent TPP-320 Polypropylene, 20% Talc Filled, Impact Modified
A. Schulman Lucent TPP-220 Polypropylene, 20% Talc Filled, Impact Modified
A. Schulman Lucent TPP-120 Polypropylene, Homopolymer, 20% Talc Filled
A. Schulman Fiberfil® PP-68/TC/20 Polypropylene Copolymer, 20% Talc

PINNO035 / 82696

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.