MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
SABIC NORYL GTX™ Resin GTX678 Polyphenylene Ether + PA (PPE+Nylon) (Europe)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Polyphenylene Ether/PPO

Material Notes: NORYL GTX™ 678 resin is a conductive, high performance non-reinforced alloy of Polyphenylene Ether (PPE) + Polyamide (PA). This injection moldable grade is optimized for primer-less electrostatic and powder coat painting, and it is UL 5VA rated with a non-brominated, non-chlorinated FR package. NORYL GTX678 resin exhibits an excellent balance of conductivity, high heat resistance, good ductility, and is heat stabilized. This material is an excellent candidate for non-automotive painted applications such as office furniture, PVC/metal replacement, lighting ballast housings / enclosures, and appliance exteriors.

Features: Hydrolytic Stability,Chemical Resistance,Good Stiffness,Low Warpage,Heat Stabilized,Conductive,Structural

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.12 g/ccASTM D792
Density 1.12 g/ccISO 1183
Moisture Absorption 0.0300 %Profile Extrusion
 0.0700 %Injection Molding
 0.500 %23°C / 50% RH; ISO 62
Water Absorption at Saturation 4.0 %ISO 62-1
Viscosity 7.0 cP
@Load 5.00 kg,
Temperature 300 °C
MVR cc/10 min; ISO 1133
Linear Mold Shrinkage, Flow 0.013 - 0.015 cm/cm
@Thickness 3.20 mm
SABIC method
Melt Flow 7.8 g/10 min
@Load 5.00 kg,
Temperature 300 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 52.0 MPa50 mm/min; ASTM D638
 52.0 MPa50 mm/min; ISO 527
Tensile Strength, Yield 58.0 MPa50 mm/min; ASTM D638
 58.0 MPa50 mm/min; ISO 527
Elongation at Break 12 %50 mm/min; ASTM D638
 12 %50 mm/min; ISO 527
Elongation at Yield 7.0 %50 mm/min; ASTM D638
 7.0 %50 mm/min; ISO 527
Tensile Modulus 2900 MPa5 mm/min; ASTM D638
 2900 MPa1 mm/min; ISO 527
Flexural Strength 95.0 MPayld, 1.3 mm/min, 50 mm span; ASTM D790
 95.0 MPayield, 2 mm/min; ISO 178
Flexural Modulus 2600 MPa1.3 mm/min, 50 mm span; ASTM D790
 2600 MPa2 mm/min; ISO 178
Izod Impact Notched 100 JASTM D256
 70.0 J
@Temperature -30.0 °C
ASTM D256
Izod Impact, Notched (ISO) 10.0 kJ/m²80*10*4; ISO 180/1A
 7.00 kJ/m²
@Temperature -30.0 °C
80*10*4; ISO 180/1A
Charpy Impact, Notched 12.0 kJ/m²Edgew 80*10*4 sp=62mm; ISO 179/1eA
Dart Drop, Total Energy 60.0 JASTM D3763
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 4000 ohm-cmASTM D257
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 78.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
 83.0 µm/m-°C
@Temperature 23.0 - 60.0 °C
ISO 11359-2
CTE, linear, Transverse to Flow 80.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
 85.0 µm/m-°C
@Temperature 23.0 - 60.0 °C
ISO 11359-2
Specific Heat Capacity 1.40 J/g-°CASTM C351
Thermal Conductivity 0.200 W/m-KASTM C177
Hot Ball Pressure Test 125 °CPASS; IEC 60695-10-2
Deflection Temperature at 0.46 MPa (66 psi) 191 °CFlatw 80*10*4 sp=64mm; ISO 75/Bf
 195 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Vicat Softening Point 195 °CRate B/120; ISO 306
 197 °CRate B/50; ISO 306
 198 °CRate B/50; ASTM D1525
 
Processing PropertiesOriginal ValueComments
Processing Temperature 40.0 - 50.0 °CWater Bath Temperature
 35.0 - 75.0 °CCalibrator Temperature
Nozzle Temperature 275 - 300 °C
Zone 1 245 - 260 °CProfile Extrusion
Zone 2 245 - 260 °CProfile Extrusion
 265 - 300 °C
Zone 3 245 - 260 °CProfile Extrusion
 270 - 300 °C
Zone 4 245 - 260 °CProfile Extrusion
Adapter Temperature 245 - 260 °CProfile Extrusion
Die Temperature 245 - 260 °CProfile Extrusion
Melt Temperature 245 - 260 °CProfile Extrusion
 275 - 300 °CInjection Molding
Mold Temperature 65.0 - 95.0 °C
Drying Temperature 95.0 - 105 °CInjection Molding
 105 - 110 °CProfile Extrusion
Dry Time 3.00 - 4.00 hourInjection Molding
 8.00 hourCumulative; Injection Molding
 8.00 hourProfile Extrusion
 24.0 hourCumulative; Profile Extrusion
Moisture Content 0.020 %minimum
Back Pressure 0.300 - 1.40 MPa
Shot Size 30 - 50 %
Vent Depth 0.00130 - 0.00380 cm
Screw Speed 20 - 100 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABH82131 / 290078

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.