MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Du-Co Ceramics Mullite
Categories: Ceramic; Oxide; Aluminum Oxide

Material Notes: Mullite is a high temperature alumino-silicate ceramic with good mechanical strength and excellent thermal shock properties due to its low thermal expansion coefficient. Mullite is a lower cost alternative to dense alumina in applications such as thermocouple applications, furnace muffle tubes, kiln rollers, sight tubes, rods and kiln furniture.

Information provided by DU-CO Ceramics Company.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 2.30 g/cc
Water Absorption 0.00 %Impervious
 
Mechanical PropertiesOriginal ValueComments
Flexural Strength 115 MPa
 
Thermal PropertiesOriginal ValueComments
CTE, linear 5.10 µm/m-°C
@Temperature 20.0 - 1000 °C
Maximum Service Temperature, Air 1500 °C
 
Descriptive Properties
ColorOff White

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Schott ZERODUR® Glass Ceramic

CDUC15 / 200160

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.