Grade for calandering; no yellowing under the action of UV light; good low-temperature flexibility; high rebound resilience; improved microbial resistance; Improved hydrolysis resistance; Application; Textile coatingAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro. |