MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Redwood Plastics Redco™ 55A Polyurethane
Categories: Polymer; Thermoset; Polyurethane, TS

Material Notes: Redco™ 55A is a pliable urethane similar to a soft rubber, but more resilient, with a balanced range of properties including excellent gripping characteristics.

Standard Color: Purple/Maroon

Features: Strong, Oil Resistant, Abrasion Resistant, Impact Resistant

Typical Applications: Dolly wheel tires, carry over tires, feed wheels, roll covers, shock and vibration pads, rollers, carry over wheels, bumpers, wheels, flexible parts, impact pads, anti-vibration parts, wipers, etc.

Information provided by Redwood Plastics and Rubber

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.19 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 52 - 58
Tensile Strength 37.0 MPa
Elongation at Break 690 %
100% Modulus 1.90 MPa
300% Modulus 3.90 MPa
Resilience 66DIN
Tear Strength 13.5 kN/mTrouser
 36.4 kN/mAngle, Die C
Abrasion 14[mm3], DIN, 10N
Compression Set 31 %Method B
 
Descriptive Properties
ColorPurple/Maroon

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PREDW027 / 296593

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.