System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
Flint Hills P9G1Z-047 Polypropylene
Categories:
Polymer
;
Thermoplastic
;
Polypropylene (PP)
;
Polypropylene, Extrusion Grade
Material Notes:
Features:
Processing stability. Product does not contain animal derived components. Phthalate-free.
Applications:
Extrusion: Thick sheeting
Information Provided by Flint Hills Resources
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Density
0.900
g/cc
ASTM D1505
Melt Flow
0.55
g/10 min
ASTM D1238
Mechanical Properties
Original Value
Comments
Hardness, Rockwell R
92
ASTM D785
Tensile Strength, Yield
34.0
MPa
ASTM D638
Elongation at Yield
14 %
ASTM D638
Flexural Modulus, 1% Secant
1170
MPa
ASTM D790
Izod Impact, Notched
91.0
J/m
@Temperature 23.0 °C
ASTM D256
Gardner Impact
29.0
J
@Temperature 23.0 °C
ASTM D5420
Tangent Modulus
1240
MPa
ASTM D790
Thermal Properties
Original Value
Comments
Deflection Temperature at 0.46 MPa (66 psi)
96.0
°C
ASTM D648
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
Users viewing this material also viewed the following:
Braskem F006EC2 Homopolymer Polypropylene
Braskem F008F Homopolymer Polypropylene
Phillips 66 COPYLENE® CH008 Polypropylene, Homopolymer, Netting
Ineos H00G-00 Polypropylene Homopolymer
Flint Hills AP5995-HA Polypropylene Impact Copolymer
PFLINT031 / 104585
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.