MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
General Plastics LAST-A-FOAM® FR-6715 Polyurethane Foam
Categories: Other Engineering Material; Composite Core Material; Polymer; Thermoset; Polyurethane, TS; Thermoset Polyurethane Foam, Unreinforced

Material Notes:

Information provided by General Plastics Manufacturing Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.240 g/ccASTM D1622
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 26.1cut foam surface; ASTM D2240
Tensile Strength 538 psiParallel to Rise; ASTM D1623
 587 psiPerpendicular to Rise; ASTM D1623
Flexural Strength 722 psiRise Parallel to Beam Thick.; ASTM D790
 859 psiRise Parallel to Test Span; ASTM D790
Flexural Modulus 24323 psiRise Parallel to Beam Thick.; ASTM D790
 27384 psiRise Parallel to Test Span; ASTM D790
Compressive Strength 276 psi
@Temperature 121 °C
Perpendicular to Rise; ASTM D1621
 282 psi
@Temperature 121 °C
Parallel to Rise; ASTM D1621
 373 psi
@Temperature 93.3 °C
Perpendicular to Rise; ASTM D1621
 439 psi
@Temperature 93.3 °C
Parallel to Rise; ASTM D1621
 732 psi
@Temperature 23.9 °C
Perpendicular to Rise; ASTM D1621
 750 psi
@Temperature 23.9 °C
Parallel to Rise; ASTM D1621
 1022 psi
@Temperature -53.9 °C
Perpendicular to Rise; ASTM D1621
 1246 psi
@Temperature -53.9 °C
Parallel to Rise; ASTM D1621
Compressive Modulus 9329 psi
@Temperature 121 °C
Perpendicular to Rise; ASTM D1621
 11820 psi
@Temperature 121 °C
Parallel to Rise; ASTM D1621
 12727 psi
@Temperature 93.3 °C
Perpendicular to Rise; ASTM D1621
 17769 psi
@Temperature 23.9 °C
Perpendicular to Rise; ASTM D1621
 19340 psi
@Temperature 93.3 °C
Parallel to Rise; ASTM D1621
 22590 psi
@Temperature 23.9 °C
Parallel to Rise; ASTM D1621
 24879 psi
@Temperature -53.9 °C
Perpendicular to Rise; ASTM D1621
 40904 psi
@Temperature -53.9 °C
Parallel to Rise; ASTM D1621
Poissons Ratio 0.30
Shear Modulus 5.988 ksiRise Parallel to Specimen Width; ASTM C273
 6.15 ksiRise Parallel to Specimen Thickness; ASTM C273
Shear Strength 0.453 ksiRise Parallel to Specimen Width; ASTM C273
 0.457 ksiRise Parallel to Specimen Thickness; ASTM C273
 
Thermal PropertiesOriginal ValueComments
CTE, linear 35.0 µin/in-°F
@Temperature -45.6 - 93.3 °C
GP Method
Specific Heat Capacity 0.376 BTU/lb-°FASTM E1269
Thermal Conductivity 0.285 BTU-in/hr-ft²-°FASTM C518
Glass Transition Temp, Tg 275 °FASTM E1824
 
Descriptive Properties
Closed Cell Content97.1%
Heat of Combustion10939 BTU/lbASTM D240
Tumbling Friability (%)4.9
Water Absorption0.036 lbs/ft²

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
General Plastics LAST-A-FOAM® FR-3703 Polyurethane Foam
General Plastics LAST-A-FOAM® FR-3710 Polyurethane Foam
General Plastics LAST-A-FOAM® FR-3708 Polyurethane Foam
General Plastics LAST-A-FOAM® FR-3706 Polyurethane Foam
General Plastics LAST-A-FOAM® FR-3704 Polyurethane Foam

PGENR042 / 186828

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.