MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Avient Bergamid™ PA66 C20 Black Polyamide 66 (Nylon 66)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66)

Material Notes: Product code EM00000364BI

Information provided by PolyOne

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.23 g/ccISO 1183
Filler Content 20 %Carbon Fiber Reinforcement
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 203 MPa
@Temperature 23.0 °C
ISO 527
Elongation at Break 2.3 %
@Temperature 23.0 °C
ISO 527
Tensile Modulus 13200 MPa
@Temperature 23.0 °C
ISO 527
Charpy Impact Unnotched 61.0 kJ/m²
@Temperature 23.0 °C
ISO 179
 
Electrical PropertiesOriginal ValueComments
Surface Resistance 1700 ohmASTM D257
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 245 °CUnannealed; ISO 75-2
Deflection Temperature at 1.8 MPa (264 psi) 235 °CUnannealed; ISO 75-2
 
Processing PropertiesOriginal ValueComments
Melt Temperature 260 - 280 °C
Mold Temperature 65.0 - 85.0 °C
Drying Temperature 80.0 - 90.0 °C
Dry Time 4.00 - 6.00 hour
 
Descriptive Properties
AppearanceBlack
FeaturesGood Dimensional Stability
 Good Impact Resistance
 Good Stiffness
FormsPellets
Generic MaterialNylon 66
Generic NamePolyamide 66 (Nylon 66)
Processing MethodInjection Molding
Regional AvailabilityAsia Pacific
 Europe
 North America

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
BASF Ultramid® 1000-11 NF2001 PA66 (Dry)
Asahi Kasei Thermylon® N3-25FG-2726 PA66-GF25
BASF Ultramid® 1310-11 NF2001 PA66 (Dry)
Envalior Durethan® A 30 S FN31 000000 Nylon 66 (PA66), Dry
Envalior Durethan® DP 2801 000000 Nylon 66 (PA66), Dry

PH0POL1432 / 146001

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.