HIFOR Xtreme® SC74869 is a hexene LLDPE designed for blown film extrusion of can liners and heavy duty films. This material contains low slip, very high anti-block, and process aid for high speed extrusion. This product has some 21 CFR clearances. Application/Uses: Blown film extrusion, Can Liners.Information provided by Westlake Chemical Corporation. |