MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Geon® Performance Solutions 2540-xx04FRD Vinyl Compound - Wire & Cable  (discontinued **)
Categories: Polymer; Thermoplastic; Vinyl (PVC); PVC, Wire and Cable Grade

Material Notes:

Description/Features:

  • UL 75°C
  • Non-migrating, Non-contaminating
  • Mil C-17, 13930 Type JP Coaxial Cable
  • Flame Retardant

Applications:

  • Telecommunication Jacket

Market:

  • Wire & Cable

Processing Method:

  • Extrusion Coating
PolyOne First Choice

Disclaimer: NOTE: Typical Properties of Molded Slab (0.075"); Not to be Construed as Specifications.

Information provided by PolyOne Corporation.

Geon Performance Solutions was created from PolyOne in 2019.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.29 g/ccASTM D792
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 8215 sec; ASTM D2240
Tensile Strength, Yield 2400 psiType 4 - Flexibles, 20 in/min; ASTM D638
Elongation at Break 360 %Type 4 - Flexibles, 20 in/min; ASTM D638
Tensile Modulus 1224 psiType 4 - Flexibles, 20 in/min; ASTM D638
 
Thermal PropertiesOriginal ValueComments
Oxygen Index 28 %0.075 in; ASTM D2863
 
Processing PropertiesOriginal ValueComments
Melt Temperature 340 - 345 °FExtrusion
 
Descriptive Properties
Immersion - Flexible Strength Change110 %ASTM Oil #2, 250°F (121°C), 18 hrs; ASTM D543
Immersion - Percent Change of Elongation0 %ASTM Oil #2, 250°F (121°C), 18 hrs; ASTM D543
Oven Aged - Retention of Elongation (ROE)80 %235°F (113°C), 168 hrs (7 days), 0.075 in; UL Standard
Oven Aged - Retention of Tensile Strength (ROT)95 %235°F (113°C), 168 hrs (7 days), 0.075 in; UL Standard
Product FormPellets/Cubes

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PH1PO1254 / 43959

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.