MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Radici Radiflam® A AE (dry) Nylon 66  (discontinued **)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Unreinforced, Flame Retardant

Material Notes: Radiflam® A is a range of flame retardant polyamides 66 (PA 66) used for injection molding and extrusion for all applications where high fire resistance is required.

Information provided by Radici group.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.20 g/cc
Water Absorption 6.2 %
Moisture Absorption at Equilibrium 1.6 %
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 70.0 MPa
Elongation at Break 5.1 %
Tensile Modulus 3550 MPa
Charpy Impact Unnotched NB
@Temperature 23.0 °C
 NB
@Temperature -30.0 °C
Charpy Impact, Notched 3.00 kJ/m²
@Temperature -30.0 °C
 3.50 kJ/m²
@Temperature 23.0 °C
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+11 ohm-cm
 
Thermal PropertiesOriginal ValueComments
Melting Point 260 °C
Deflection Temperature at 0.46 MPa (66 psi) 210 °C
Deflection Temperature at 1.8 MPa (264 psi) 75.0 °C
Vicat Softening Point 220 °C
@Load 5.10 kg
50°C/h
Flammability, UL94 V-0
@Thickness 1.60 mm
 V-0
@Thickness 0.800 mm

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Radici Radilon® A RV150 (cond.) Nylon 66
Radici Radiflam® BN100 AE Polybutylene Terephthalate
Radici Radiflam® ARV300 AE (dry) Nylon 66
Radici Radiflam® A FR (cond.) Nylon 66
Covestro Bayblend® FR3000 PC/ABS Blend

PRADI778 / 120291

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.