System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
Mocom (ALBIS) Altech® A 1000/110 IM PA6, Dry
Categories:
Polymer
;
Thermoplastic
;
Nylon (Polyamide PA)
;
Nylon 6 (PA6)
;
Nylon 6, Unreinforced
Material Notes:
Polyamide 6; high impact modified, dry impact modified, easy release (demolding), high flow. Applications: housings, various
Information provided by ALBIS.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Density
1.11
g/cc
ISO 1183
Linear Mold Shrinkage, Flow
0.012
-
0.014
cm/cm
@Time 86400 sec
ISO 294-4
Linear Mold Shrinkage, Transverse
0.010
-
0.012
cm/cm
@Time 86400 sec
ISO 294-4
Melt Flow
12
g/10 min
@Load 2.16 kg,
Temperature 235 °C
cm3/10min, volumetric value; ISO 1133
Mechanical Properties
Original Value
Comments
Tensile Strength, Yield
65.0
MPa
ISO 527-1/-2
Elongation at Yield
3.5 %
ISO 527-1/-2
Tensile Modulus
2600
MPa
ISO 527-1/-2
Flexural Strength
85.0
MPa
ISO 178
Flexural Modulus
2300
MPa
ISO 178
Charpy Impact Unnotched
NB
ISO 179/1eU
Charpy Impact, Notched
12.0
kJ/m²
ISO 179/1eA
Thermal Properties
Original Value
Comments
Melting Point
220
°C
ISO 11357
Deflection Temperature at 1.8 MPa (264 psi)
60.0
°C
ISO 75-1/-2
Vicat Softening Point
185
°C
B50; ISO 306
Flammability, UL94
HB
@Thickness 1.50 mm
Processing Properties
Original Value
Comments
Melt Temperature
250
-
270
°C
injection molding
Mold Temperature
40.0
-
80.0
°C
injection molding
Drying Temperature
80.0
°C
@Time 7200 - 43200 sec
in desiccant dryer, depends on moisture content
Moisture Content
<= 0.0015 %
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
Users viewing this material also viewed the following:
A. Schulman ComAlloy Hiloy® 612 Nylon 6, Glass Reinforced, UL
Asahi Kasei Leona™ 13G15 Polyamide 66, GF Reinforced
Mitsubishi Chemical Advanced Materials Nylatron® MD PA6, Metal-detectable Nylon (ASTM Product Data Sheet)
NYCOA NY-FLEX® CT 145 Nylon-Based TPE
A. Schulman ComAlloy Hiloy® 613 Nylon 6, Glass Reinforced, UL
PALBIS9910 / 221006
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.