MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
SABIC CYCOLOY™ MC8100 PC+ABS (Asia)
Categories: Polymer; Thermoplastic; ABS Polymer; Polycarbonate/ABS Alloy, Unreinforced

Material Notes: PC/ABS, extrusion and blow molding grade.

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.13 g/ccASTM D792
Water Absorption 0.10 %24 hours; ASTM D570
Moisture Absorption at Equilibrium 0.40 %ASTM D570
Linear Mold Shrinkage, Flow 0.0040 - 0.0070 cm/cm
@Thickness 3.20 mm
SABIC method
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 52.0 MPa50 mm/min; ASTM D638
Elongation at Break 100 %50 mm/min; ASTM D638
Elongation at Yield 5.0 %50 mm/min; ASTM D638
Tensile Modulus 2060 MPa50 mm/min; ASTM D638
Flexural Yield Strength 77.0 MPa1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 2060 MPa1.3 mm/min, 50 mm span; ASTM D790
Izod Impact, Notched 534 J/mASTM D256
 427 J/m
@Temperature -30.0 °C
ASTM D256
Dart Drop, Total Energy 54.0 JASTM D3763
 47.0 J
@Temperature -30.0 °C
ASTM D3763
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 81.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
Thermal Conductivity 0.200 W/m-KASTM C177
Deflection Temperature at 0.46 MPa (66 psi) 123 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 104 °C
@Thickness 3.20 mm
unannealed; ASTM D648
 
Processing PropertiesOriginal ValueComments
Feed Temperature 60.0 - 80.0 °C
Zone 1 240 - 250 °CExtrusion Blow Molding
Zone 2 240 - 255 °CExtrusion Blow Molding
Zone 3 240 - 255 °CExtrusion Blow Molding
Zone 4 240 - 255 °CExtrusion Blow Molding
Zone 5 245 - 260 °C
Die Temperature 250 - 265 °CExtrusion Blow Molding
Melt Temperature 245 - 260 °C
Head Temperature 245 - 260 °CZone 6 - Top Temperature
 245 - 260 °CZone 7 - Bottom Temperature
Mold Temperature 40.0 - 90.0 °C
Drying Temperature 100 - 110 °CExtrusion Blow Molding
Dry Time 3.00 - 4.00 hourExtrusion Blow Molding
 24.0 hourCumulative; Extrusion Blow Molding
Moisture Content >= 0.040 %
 0.040 - 0.050 %
Screw Speed 20 - 50 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABI10764 / 244231

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.