MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Teknor Apex Monprene® RG-13271 Thermoplastic Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Notes: Monprene RG-13271 is specifically designed for food contact applications and other regulated markets such as children’s and infants products. Every ingredient used to formulate Monprene RG-13271 is either “generally recognized as safe” (GRAS), prior sanctioned, subject to an effective Food Contact Notification (FCN), subject to a Threshold of Regulation (TOR) or identified in one or more section of Title 21 of the code of Federal Regulations published by the US FDA. This product is suitable for injection molding.

Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America

Features: Filled; Food Contact Acceptable; Medium Density; Medium Flow; Medium Hardness; Slip

Uses: Consumer Applications; Gaskets; Handles; Kitchenware; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments

RoHS Compliance: RoHS Compliant

Form: Pellets

Processing Method: Injection Molding

Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.01 g/cc
Melt Flow 4.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 71
@Time 5.00 sec
Injection Molded; ASTM D2240
 73
@Time 1.00 sec
Injection Molded; ASTM D2240
Tensile Strength at Break 994 psiDie C, 20 in/min, Flow; ASTM D412
 1570 psiDie C, 20 in/min, Across Flow; ASTM D412
Tensile Stress at Strain 314 psi
@Strain 100 %
Die C, 20 in/min, Across Flow; ASTM D412
 445 psi
@Strain 300 %
Die C, 20 in/min, Across Flow; ASTM D412
 649 psi
@Strain 300 %
Die C, 20 in/min, Flow; ASTM D412
 688 psi
@Strain 100 %
Die C, 20 in/min, Flow; ASTM D412
Elongation at Break 550 %Die C, 20 in/min, Flow; ASTM D412
 790 %Die C, 20 in/min, Across Flow; ASTM D412
Tear Strength 172 pliDie C, 20 in/min, Flow; ASTM D624
 185 pliDie C, 20 in/min, Across Flow; ASTM D624
Compression Set 71 %
@Temperature 70.0 °C,
Time 79200 sec
Type 1; ASTM D395B
 73 %
@Temperature 22.8 °C,
Time 79200 sec
Type 1; ASTM D395B
 
Processing PropertiesOriginal ValueComments
Processing Temperature 370 - 410 °FMelt, Injection
Rear Barrel Temperature 340 - 380 °FInjection
Middle Barrel Temperature 350 - 390 °FInjection
Front Barrel Temperature 360 - 400 °FInjection
Nozzle Temperature 370 - 410 °FInjection
Zone 1 330 - 370 °FExtrusion
Zone 2 340 - 380 °FExtrusion
Zone 3 350 - 390 °FExtrusion
Zone 5 360 - 400 °FExtrusion
Die Temperature 374 - 410 °FExtrusion
Mold Temperature 77.0 - 150 °FInjection
Injection Pressure 200 - 1000 psiInjection
Back Pressure 25.0 - 50.0 psiInjection
Cushion 0.150 - 1.00 inInjection
Screw Speed 30 - 100 rpmExtrusion
 50 - 100 rpmInjection
 
Descriptive Properties
AppearanceOpaque

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PTEKNQ0925 / 237416

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.