MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Fibre Glast Duratec 1040 Clear Hi-Gloss Gel Coat Additive
Categories: Polymer; Thermoset; Polyester, TS; Polyester (Thermoset) - Rigid

Material Notes: #1040 can be mixed 1:1 with regular gel coat to reduce viscosity, porosity, and permit a complete open air cure. The reduction in viscosity allows gel coat to be sprayed controllably through siphon and HVLP equipment, reducing sanding and polishing time. Below the waterline repairs still need the addition of #71 Styrene Wax for maximum hardness.

Features:
  • Low Porosity - when used for repairs, blending the additive with gelcoat produces a low porosity surface
  • Reduced orange peel - the low viscosity of the blend results in a smooth finish that is easily sanded
  • Improved properties - for mold surfaces, the blending of the additive with tooling gelcoat creates a higher heat distortion temperature, improved gloss retention, increased impact resistance and reduced subsurface porosity.
  • Superior Finish - when blended one-to-one with gelcoats, the additive created an air-cure enamel-like coating. No air-dry additive is required. When used for gelcoat repair, surfaces are restored to like-new condition.

    Information provided by Fibre Glast Developments Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Brookfield Viscosity 110 cPBrookfield RVF #2 Spindle at 20 rpm
 
Optical PropertiesOriginal ValueComments
Transmission, Visible 90 %clear; thickness not quantified
 
Processing PropertiesOriginal ValueComments
Gel Time 16.0 - 20.0 minValue for a 100g mass, catalyzed at 2 percent with MEKP - 2%

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Dow 3-4170 DIELECTRIC GEL KIT
Wacker Lumisil® LR 7601/80 Liquid Silicone Rubber
C.O.I.M. EXTER S® S 103 L Orthophthalic Resin
BCC Products BC 9040 T Silicone RTV Rubber
Aremco Heat-Away™ 641-EV Thermally Conductive Grease, Silver Filled, for High Vacuum Systems

PFIBRE42 / 38302

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.