Multi-Flex® high heat compounds are a new generations elastomers exhibiting improved compression set at elevated temperature. Multi-Flex® TPE compounds are based on Kraton G technology and feature excellent heat and ozone resistance. These products cover a wide temperature span from -50°C to 150°C. Multi-Flex TPE contains Kraton™ G. Data provided by Multibase. |