High Performance Light-Curing Adhesives and Coatings for Electronic AssemblyDymax 9-984-B Conformal Coating Cures to an opaque black finish; hides components or circuitry from view; protects sensitive circuits from light. Cure Speed (fpm): 2 - 6 Cure Type: UV, Visible and Heat |