MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.

(Viewing data as-entered. Click here to return)
Ineos Nova 331 Impact Polystyrene  (discontinued **)
Categories: Polymer; Thermoplastic; Polystyrene (PS)

Material Notes: Features: High Flow, specially formulated for high speed equipment, allows lighter weight part designs, designed for use in thin wall or long flow path moldings, USP Class VI.

Uses: Packaging, housewares, toys, cutlery, and medical.

Property data below are typical values determined from injection molded samples at 23°C and 50% RH.

INEOS NOVA began October 1 2007 as an expansion of the 50:50 joint venture between NOVA Chemicals and INEOS to include North American assets. 

Key Words: Nova Styrenics
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.04 g/ccASTM D792
Linear Mold Shrinkage 0.0040 - 0.0070 cm/cmASTM D955
Melt Flow 15.5 g/10 minCondition G; ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 29.0 MPaASTM D638
Elongation at Break 35 %ASTM D638
Flexural Yield Strength 35.0 MPaASTM D790
Flexural Modulus 2.14 GPaASTM D790
Izod Impact, Notched 0.900 J/cm1/8 in. bar; 0.010 in. notch radius; ASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 82.0 °CAnnealed; ASTM D648
Vicat Softening Point 91.0 °CASTM D1525
 
Compliance PropertiesOriginal ValueComments
USP Class VI Yes

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Ineos 3950 Polypropylene Impact Copolymer
DuPont Mobility and Materials Zytel® ST801 BK010A PA66-HI
Celanese Zytel® ST801 NC010A PA66-HI

PSTN32 / 69227

USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.