MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Teknor Apex Sarlink® TPV 4190 Thermoplastic Vulcanizate
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Vulcanizate Elastomer (TPV)

Material Notes: Notes: Sarlink TPV 4100 series are engineered materials designed primarily for demanding automotive and industrial applications. Available in both black and natural, this product is a low density, higher hardness thermoplastic vulcanizate featuring excellent flex fatigue resistance, heat aging, improved elasticity and resilience. It can be used in injection molded parts, sheet and profile extrusion such as weather-stripping and expansion joints, and can also be blow molded into boots and ducts.

Availability: Asia Pacific; Europe; Latin America; North America

Features: Chemical Resistant; Excellent Elastic Recovery; Fatigue Resistant; Good Adhesion; Good Flexibility; Good Melt Strength; Good Moldability; Good Processability; Good Surface Finish; Heat Aging Resistant; High Hardness; High Melt Stability; Low Density; Low Specific Gravity; Low Temperature Flexibility; Medium Heat Resistant; Resilient

Uses: Agricultural Applications; Appliance Components; Automotive Applications; Automotive Exterior Parts; Automotive Interior Parts; Automotive Under the Hood; Blow Molding Applications; Gaskets; Industrial Applications; Pipe Seals; Profiles; Rubber Replacement; Sheet; Weatherstripping; White Goods & Small Appliance

Agency Ratings: UL 94

RoHS Compliance: RoHS Compliant

Automotive Specifications: CHRYSLER MS-AR-100 EGN Color: Black; CHRYSLER MS-AR-100 EGN Color: Natural; FORD WSD-M2D382-A1 Color: Black; FORD WSD-M2D382-A1 Color: Natural; GM GMP.E/P.005 Color: Black; GM GMP.E/P.005 Color: Natural; GM GMW/15813 Type 8 Color: Black; GM GMW/15813 Type 8 Color: Natural; GM QK 3526 Type 6 Color: Black; GM QK 3526 Type 6 Color: Natural

UL File Number: QMFZ2. E54709

Form: Pellets

Processing Method: Extrusion; Injection Molding; Blow Molding

Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.950 g/ccISO 1183
Viscosity 340 cP
@Shear Rate 206 1/s,
Temperature 200 °C
Shear, Capillary; ASTM D3835
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 86
@Time 5.00 sec
Extruded; ASTM D2240
 90
@Time 5.00 sec
Injection Molded; ASTM D2240
Tensile Strength at Break 1970 psiFlow; ASTM D412
 2100 psiAcross Flow; ASTM D412
 1870 psi
@Treatment Temp. 135 °C,
Time 3.60e+6 sec
Across Flow, Change in Air; ISO 188
 1930 psi
@Treatment Temp. 150 °C,
Time 605000 sec
Across Flow, Change in Air; ISO 188
Tensile Stress at Strain 972 psi
@Strain 100 %
Across Flow; ISO 37
 1480 psi
@Strain 100 %
Flow; ISO 37
 1070 psi
@Strain 100 %,
Treatment Temp. 150 °C
Across Flow, Change in Air at 168 hr; ISO 188
 1120 psi
@Strain 100 %,
Treatment Temp. 135 °C
Across Flow, Change in Air at 1000 hr; ISO 188
Elongation at Break 380 %Flow; ASTM D412
 650 %Across Flow; ASTM D412
 540 %
@Treatment Temp. 150 °C,
Time 605000 sec
Across Flow, Change in Air; ISO 188
 546 %
@Treatment Temp. 135 °C,
Time 3.60e+6 sec
Across Flow, Change in Air; ISO 188
Poissons Ratio 0.43ASTM E132
Tear Strength 410 pliMethod Ba, Angle (Unnicked); ISO 34-1
Compression Set 36 %
@Temperature 22.8 °C,
Time 79200 sec
ISO 815
 48 %
@Temperature 70.0 °C,
Time 79200 sec
ISO 815
 72 %
@Temperature 125 °C,
Time 252000 sec
ISO 815
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 2.39
@Thickness 2.00 mm
ASTM D150
Dielectric Strength 520 V/mil
@Thickness 2.00 mm
ASTM D419
 
Thermal PropertiesOriginal ValueComments
Flammability, UL94 HB
@Thickness 1.02 mm
All Colors
 
Processing PropertiesOriginal ValueComments
Processing Temperature 360 - 440 °FInjection
Rear Barrel Temperature 280 - 320 °FInjection
Middle Barrel Temperature 330 - 380 °FInjection
Front Barrel Temperature 350 - 440 °FInjection
Nozzle Temperature 360 - 440 °FInjection
Zone 1 356 - 392 °FExtrusion
Zone 2 356 - 401 °FExtrusion
Zone 3 369 - 410 °FExtrusion
Zone 4 369 - 410 °FExtrusion
Die Temperature 383 - 419 °FExtrusion
Melt Temperature 383 - 419 °FExtrusion
Mold Temperature 60.0 - 130 °FInjection
Drying Temperature 180 °F
Dry Time 3.00 hour
Screw Speed 25 - 75 rpmInjection
 
Descriptive Properties
AppearanceBlack
 Natural Color
 Opaque

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ExxonMobil Santoprene® 8123-45S100 Thermoplastic Elastomer

PTEKNQ1161 / 237652

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.