MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
SABIC CYCOLAC™ EX58 ABS (Asia)
Categories: Polymer; Thermoplastic; ABS Polymer

Material Notes: High impact ABS for sheet extrusion and blow molding applications.

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.03 g/ccASTM D792
Density 1.03 g/ccISO 1183
Viscosity 1.55e+6 cP
@Shear Rate 100 1/s,
Temperature 240 °C
melt; ASTM D3825
Linear Mold Shrinkage, Flow 0.0060 - 0.0080 cm/cm
@Thickness 3.20 mm
SABIC method
Melt Flow 4.0 g/10 min
@Load 10.0 kg,
Temperature 220 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 102ASTM D785
Tensile Strength at Break 30.0 MPa50 mm/min; ISO 527
 30.0 MPa5 mm/min; ASTM D638
Tensile Strength, Yield 39.0 MPa5 mm/min; ASTM D638
 41.0 MPa50 mm/min; ISO 527
Elongation at Break 21 %50 mm/min; ISO 527
 32 %5 mm/min; ASTM D638
Elongation at Yield 2.6 %50 mm/min; ISO 527
 3.1 %5 mm/min; ASTM D638
Tensile Modulus 1970 MPa1mm/min; ISO 527
 2080 MPa5 mm/min; ASTM D638
Flexural Yield Strength 60.0 MPa2 mm/min; ISO 178
 66.0 MPa1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 2000 MPa2 mm/min; ISO 178
 2160 MPa1.3 mm/min, 50 mm span; ASTM D790
Izod Impact, Notched 432 J/mASTM D256
 299 J/m
@Temperature -30.0 °C
ASTM D256
Izod Impact, Notched (ISO) 35.0 kJ/m²80*10*4; ISO 180/1A
 23.0 kJ/m²
@Temperature -30.0 °C
80*10*4; ISO 180/1A
Charpy Impact, Notched 37.0 kJ/m²Edgew 80*10*4 sp=62mm; ISO 179/1eA
Dart Drop, Total Energy 37.0 JASTM D3763
 
Electrical PropertiesOriginal ValueComments
Arc Resistance 120 - 180 secASTM D495
Comparative Tracking Index >= 600 VUL 746A
Hot Wire Ignition, HWI 7.0 - 15 secUL 746A
High Amp Arc Ignition, HAI 0.00 - 15 arcsUL 746A
High Voltage Arc-Tracking Rate, HVTR 10.0 - 25.4 mm/minUL 746A
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 101 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
CTE, linear, Transverse to Flow 104 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
Deflection Temperature at 0.46 MPa (66 psi) 91.0 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 78.0 °CFlatw 80*10*4 sp=64mm; ISO 75/Af
 76.0 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Vicat Softening Point 95.0 °CRate B/50; ISO 306
 97.0 °CRate B/120; ISO 306
 106 °CRate B/50; ASTM D1525
UL RTI, Electrical 60.0 °CUL 746B
UL RTI, Mechanical with Impact 60.0 °CUL 746B
UL RTI, Mechanical without Impact 60.0 °CUL 746B
Flammability, UL94 HB
@Thickness 1.50 mm
UL 94
 
Processing PropertiesOriginal ValueComments
Feed Temperature 60.0 - 75.0 °C
Zone 1 170 - 200 °CSheet Extrusion
 205 - 225 °CExtrusion Blow Molding
Zone 2 180 - 220 °CSheet Extrusion
 205 - 225 °CExtrusion Blow Molding
Zone 3 190 - 225 °CSheet Extrusion
 205 - 225 °CExtrusion Blow Molding
Zone 4 205 - 225 °CExtrusion Blow Molding
 200 - 240 °CSheet Extrusion
Zone 5 210 - 230 °C
Adapter Temperature 205 - 250 °CSheet Extrusion
Die Temperature 215 - 235 °CExtrusion Blow Molding
 205 - 250 °CSheet Extrusion
Melt Temperature 215 - 230 °C
 215 - 260 °C
Head Temperature 215 - 230 °CZone 6 - Top Temperature
 215 - 230 °CZone 7 - Bottom Temperature
Mold Temperature 40.0 - 80.0 °C
Roll Temperature 90.0 - 95.0 °CRoll Stack Temp - Top
 95.0 - 105 °CRoll Stack Temp - Middle
 100 - 105 °CRoll Stack Temp - Bottom
Drying Temperature 80.0 - 90.0 °CExtrusion Blow Molding
 80.0 - 95.0 °CSheet Extrusion
Dry Time 4.00 hourSheet Extrusion
 4.00 - 5.00 hourExtrusion Blow Molding
 24.0 hourCumulative; Extrusion Blow Molding
Moisture Content 0.020 %
 0.020 %
Screw Speed 20 - 60 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABI10019 / 243486

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.