Notes: Monprene CP-18152 CLR is a high performance thermoplastic elastomer designed for a variety of industrial and consumer product applications requiring a soft, rubber-like feel. Monprene CP-18152 CLR is a low density, low hardness, RoHS compliant grade that is suitable for injection molding. Availability: Africa & Middle East; Europe; Asia Pacific; Latin America; North America Features: General Purpose; Good Adhesion; Good Colorability; Good Moldability; Good Tear Strength; Good Tensile Strength; High Clarity; High Elongation; High Flow; High Toughness; Low Density; Low Specific Gravity; Slip; Low Hardness; Without Fillers Uses: Consumer Applications; Flexible Grip; General Purpose; Industrial Applications; Rubber Replacement; Toys RoHS Compliance: RoHS Compliant Form: Pellets Processing Method: Injection Molding Preliminary data. Information provided by Teknor Apex |