MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Huntsman IROGRAN® A 94 E 4900 TPU-Polyester
Categories: Polymer; Thermoplastic; Polyurethane, TP; Thermoplastic Polyurethane (TPUR), Polyester Grade

Material Notes: Introduction: IROGRAN A 94 E 4900 is a thermoplastic polyester polyurethane for melt calendering. IROGRAN is part of the HUNTSMAN technical extrusion/injection molding product range and offers a specially designed, flexible material with a broad processing window.

Performance Features:

  • High oil resistance
  • High production rate
  • Good melt flow
  • Easy coloring
Applications:
  • Calendering
  • Technical molding

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.22 g/ccInjection molded parts; ASTM D792
Melt Index of Compound 60 g/10 min
@Load 10.0 kg,
Temperature 210 °C
MVR, [cm3/10 min]
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 94Injection molded parts; ASTM D2240
Hardness, Shore D 44Injection molded parts; ASTM D2240
Tensile Strength at Break 38.0 MPaInjection molded parts; DIN 53504
Elongation at Break 550 %Injection molded parts; DIN 53504
100% Modulus 0.0110 GPa
@Strain 100 %
Injection molded parts; DIN 53504
300% Modulus 0.0170 GPa
@Strain 300 %
Injection molded parts; DIN 53504
Tear Strength 571 pliInjection molded parts; DIN 53515
Abrasion 33mm3, Injection molded; DIN 53516
 
Thermal PropertiesOriginal ValueComments
Melting Point 158 - 221 °C0.025" extruded film
 
Processing PropertiesOriginal ValueComments
Feed Temperature 170 °CExtrusion
Middle Barrel Temperature 175 °CExtrusion
Adapter Temperature 180 °CExtrusion
Die Temperature 180 °CExtrusion
Roll Temperature 168 °CFront, 29 rpm
 168 °CRear, 25 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Huntsman IROGRAN® A 92 E 4670 TPU-Polyester
Huntsman IROGRAN® A 92 E 4860 TPU-Polyester
Huntsman IROGRAN® A 80 H 4698 Polyester-Based TPU-Injection Molding Grade
Huntsman IROGRAN® A 95 P 5003 TPU-Polyether
Huntsman IROGRAN® A 92 H 4656 Polyester-Based TPU-Injection Molding Grade

PHUQ105 / 159478

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.