MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
3M Dyneon™ THV 815GZ Fluorothermoplastic Granules
Categories: Polymer; Thermoplastic; Fluoropolymer

Material Notes: Dyneon THV 815 GZ provides a balance of low permeation, thermal stability, and melt processability. IT can be used to prepare molded parts and extruded films, tubes, profiles, and wire coatings. It is useful for applications that require flexibility and good chemical resistance. This product processes at higher temperature than that of previous THV grades; therefore, the use of corrosion-resistant equipment is suggested.

Information provided by Dyneon, A 3M Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Melt Index of Compound 12 g/10 min
@Load 5.00 kg,
Temperature 265 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 29.0 MPaASTM D638
Elongation at Break 420 %ASTM D638
Flexural Modulus 0.525 GPaASTM D790
 
Thermal PropertiesOriginal ValueComments
Melting Point 225 °CASTM D4591
 
Descriptive Properties
FormPellets

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
3M Dyneon™ THV 221GZ Fluoroplastic Granules
3M Dyneon™ THV 221AZ Fluoroplastic Agglomerate
3M Dyneon™ THV 500GZ Fluorothermoplastic Granules
3M Dyneon™ THV 610GZ Fluoroplastic Granules
3M Dyneon™ THV 220G Fluorothermoplastic

PDYNE028 / 34836

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.