MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
SABIC NORYL™ Resin SE1GFN1 Polyphenylene Ether + PS (PPE+PS) (Americas)
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene + Polyphenylene Ether, Unreinforced

Material Notes: NORYL™ SE1GFN1 resin is a 10% glass reinforced blend of polyphenylene ether (PPE) + high impact polystyrene (HIPS). This injection moldable grade contains non-brominated, non-chlorinated flame retardant and carries a UL94 flame rating of V1 at 1.5mm along with UL746C Outdoor Suitability rating of F1 and RTI 110C. NORYL SE1GFN1 exhibits high heat resistance, good dielectric strength, dimensional stability, hydrolytic stability, and very low moisture absorption. This material is an excellent candidate for appliance internals, indoor and outdoor electrical enclosures / housings / connectors.

Features: Hydrolytic Stability,Low Creep Sensitivity,Flame Retardant,Good Stiffness,Non-Halogenated,Non-Chlorinated,Low Warpage,Structural

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.16 g/ccASTM D792
Water Absorption 0.070 %
@Time 86400 sec
ASTM D570
Moisture Absorption 0.0200 %Injection Molding
Water Absorption at Saturation 0.22 %ASTM D570
Linear Mold Shrinkage, Flow 0.0030 - 0.0050 cm/cm
@Thickness 3.20 mm
SABIC method
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell L 104ASTM D785
Tensile Strength at Break 74.0 MPa5 mm/min; ASTM D638
Elongation at Break 5.0 %5 mm/min; ASTM D638
Flexural Strength 119 MPabrk, 1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 3990 MPa1.3 mm/min, 50 mm span; ASTM D790
Izod Impact Notched 96.0 JASTM D256
 69.0 J
@Temperature -40.0 °C
ASTM D256
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+15 ohm-cmASTM D257
Dielectric Constant 3.0
@Frequency 1e+6 Hz
ASTM D150
 3.0
@Frequency 50.0 - 60.0 Hz
ASTM D150
Dissipation Factor 0.0016
@Frequency 1e+6 Hz
ASTM D150
 0.0017
@Frequency 50.0 - 60.0 Hz
ASTM D150
Comparative Tracking Index 250 - 400 VUL 746A
Hot Wire Ignition, HWI 60 - 120 sec
@Thickness >=1.50 mm
UL 746A
 >= 120 sec
@Thickness >=1.50 mm
UL 746A
High Amp Arc Ignition, HAI 30 - 60 arcs
@Thickness >=1.50 mm
UL 746A
 60 - 120 arcs
@Thickness >=1.50 mm
UL 746A
High Voltage Arc-Tracking Rate, HVTR >= 150 mm/minUL 746A
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 131 °C
@Thickness 6.40 mm
unannealed; ASTM D648
Vicat Softening Point 147 °CRate B/50; ASTM D1525
UL RTI, Electrical 110 °CUL 746B
UL RTI, Mechanical with Impact 105 °CUL 746B
UL RTI, Mechanical without Impact 110 °CUL 746B
Flammability, UL94 V-1
@Thickness >=1.50 mm
UL 94
Oxygen Index 33.9 %ASTM D2863
 
Processing PropertiesOriginal ValueComments
Nozzle Temperature 280 - 310 °C
Zone 2 260 - 305 °C
Zone 3 270 - 310 °C
Melt Temperature 280 - 310 °CInjection Molding
Mold Temperature 75.0 - 105 °C
Drying Temperature 105 - 110 °CInjection Molding
Dry Time 3.00 - 4.00 hourInjection Molding
 8.00 hourCumulative; Injection Molding
Back Pressure 0.300 - 0.700 MPa
Shot Size 30 - 70 %
Screw Speed 20 - 100 rpm
 
Descriptive Properties
UV-light, water exposure/immersionF1UL 746C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABH82465 / 290412

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.