MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Master Bond EP110F8-3 Two component, high performance epoxy
Categories: Polymer; Thermoset; Epoxy; Epoxy Encapsulant, Unreinforced

Material Notes: Key Features:
  • Toughened system
  • Low viscosity and long working life
  • Outstanding electrical insulation properties
  • Very resistant to thermal cycling and shock
Master Bond EP110F8-3 is a two component high performance epoxy resin system with a long pot life (at least 2-3 days at room temperature). It is used primarily for potting, sealing, encapsulating and casting. This low viscosity system has a convenient and very forgiving one to two mix ratio by weight. It requires an elevated temperature cure at 250-300°F. A typical cure schedule would be 4-6 hours at 250-300°F. For optimum properties, a post cure of 3-5 hours at 350°F is recommended. Even without the optional post cure, EP110F8-3 will perform very well. EP110F8-3 has no solvents or diluents and has low shrinkage upon cure. It adheres well to a wide variety of substrates, including metals, composites, glass and many plastics. It has superior electrical insulation properties. Its physical strength properties of low tensile strength, lower modulus and relatively higher elongation, translates into a special capability to resist severe thermal cycling and shock. It has good resistance to water, oils and fuels. The color of Part A is clear while the color of Part B is amber. The service temperature range is -100°F to +300°F. It can be used in applications where very high performance electrical insulation properties and resistance to rigorous thermal cycling is needed.

Product Advantages:

  • Low viscosity liquid; flows easily
  • Long working life at room temperature
  • Outstanding thermal shock resistance
  • Very high elongation
  • Unsurpassed electrical insulation properties

Information provided by Masterbond.

Vendors: Master Bond is a leading manufacturer of adhesives, sealants, coatings and potting compounds. Master Bond’s vast product line consists of over 3,000 epoxy, polyurethane, silicone, cyanoacrylate and latex adhesives that vary in viscosity, cure speed, strength, chemical resistance, electrical properties, etc. Our custom adhesives offer design flexibility and provide excellent bonding performance. Visit www.masterbond.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Viscosity 1000 - 2000 cPmixed
 1500 - 3500 cPPart B
 6000 - 8000 cPPart A
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 40 - 50
Tensile Strength 500 - 1500 psi
Elongation at Break 120 - 150 %
Tensile Modulus 5000 - 15000 psi
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+15 ohm-cm
Dielectric Constant 2.44
@Frequency 1e+6 Hz
 2.67
@Frequency 1000 Hz
 
Thermal PropertiesOriginal ValueComments
CTE, linear 135 - 150 µm/m-°C
Maximum Service Temperature, Air 300 °F
Minimum Service Temperature, Air -100 °F
 
Processing PropertiesOriginal ValueComments
Cure Time 3.00 - 5.00 hour
@Temperature 177 °C
Optional post cure
 4.00 - 6.00 hour
@Temperature 121 - 149 °C
Shelf Life 12.0 MonthIn original unopened containers
 
Descriptive Properties
Mixing Ratio1:2Parts A to B, by weight

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Master Bond EP37-3FLF Low Exotherm Highly Flexible Two Component Epoxy

PMASTM723 / 233780

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.