MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Teknor Apex Monprene® RG-20180 Thermoplastic Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Notes: Monprene RG-20100 series is group of high performance thermoplastic elastomer specifically designed for extruded regulated applications including food contact, toys and children’s products. Monprene RG-20180 is a low density, high hardness grade that complies with various US FDA and European regulations and directives for food contact and toy safety and is suitable for extrusion.

Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America

Features: BPA Free, Food Contact Acceptable; Good Adhesion; Good Colorability; Good Processability; Low Flow; Low Density; Low Specific Gravity; Lubricated; High Hardness; No Animal Derived Components; Slip; Without Fillers

Uses: Consumer Applications; Cosmetic Packaging; Food Containers; Food Packaging; Food Service Applications; Kitchenware; Lids; Non-specific Food Applications; Rubber Replacement; Toys

RoHS Compliance: RoHS Compliant

Form: Pellets

Processing Method: Extrusion

Preliminary data. Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.880 g/ccISO 1183
Viscosity 303 cP
@Shear Rate 206 1/s,
Temperature 200 °C
ASTM D3835
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 80
@Time 5.00 sec
ISO 868
Tensile Strength at Break 1020 psi20 in/min, Flow; ASTM D412
 1740 psi20 in/min, Across Flow; ASTM D412
Tensile Stress at Strain 406 psi
@Strain 100 %
20 in/min, Across Flow; ASTM D412
 870 psi
@Strain 100 %
20 in/min, Flow; ASTM D412
Elongation at Break 250 %20 in/min, Flow; ASTM D412
 780 %20 in/min, Across Flow; ASTM D412
Compression Set 23 %
@Temperature 22.8 °C,
Time 79200 sec
Type A; ISO 815
 35 %
@Temperature 70.0 °C,
Time 79200 sec
Type A; ISO 815
 
Processing PropertiesOriginal ValueComments
Zone 1 300 - 320 °F
Zone 2 320 - 400 °F
Zone 3 340 - 420 °F
Zone 4 360 - 440 °F
Die Temperature 360 - 440 °F
 
Descriptive Properties
AppearanceColors Available
 Translucent

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PTEKNQ0944 / 237435

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.