MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Borealis LE0151 Easy Strippable Semiconductive Insulation Shield for Medium Voltage Power Cables  (discontinued **)
Categories: Polymer; Thermoplastic; Polyolefin; Polyolefin, Wire/Cable Grade

Material Notes: LE0515 is an easy strippable crosslinkable semi conductive insulation shield compound designed for medium voltage (5kV-46kV) power cable applications. Application: LE0515 is especially suitable for use in triple extrusion processes. Strip forces in the range of 0.85 – 2.15 kN/m (2-5 lbs/0.5” have been found on cables from dry cure vulcanization lines. Stripping of LE0515 from the surface of the insulation is readily initiated, and it continues easily over a wide range of temperatures without tearing. It leaves a clean insulation surface. Specifications: IEC 60502; BS 6622; NF C33-223/UTE C33-223/NF C33-226; AEIC CS 8-00; ICEA S-94-649; and ICEA S-97-682.

Information provided by Borealis AG

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.15 g/ccASTM D1928C/D 792
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 9.90 MPaafter aging 7 days @ 136°C
 11.0 MPaASTM D412
Elongation at Break >= 100 %after aging 7 days @ 136°C
 250 %ASTM D412
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 100 ohm-cm
@Temperature 23.0 °C
ASTM D991
 100 ohm-cm
@Temperature 90.0 °C
ASTM D991
 
Processing PropertiesOriginal ValueComments
Zone 1 49.0 °C
Zone 2 82.0 °C
Zone 3 93.0 °C
Zone 4 104 °C
Die Temperature 115 °C
Die Cooling Temperature 25.0 °Chopper cooling

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Borealis Borlink™ LE0315 Polyethylene Compound, Crosslinkable, Semiconductive
Borealis Borlink™ LE0595-07 Polyethylene Compound, Crosslinkable, Semiconductive
Borealis Superclean™ LR4201S Crosslinkable Polyethylene Insulation for Medium and High Voltage Power Cables
Overview of materials for Polyolefin, Wire/Cable Grade
AlphaGary Garaflex™ O 9949 RA Olefinic Thermoplastic Elastomer

PBOREA507 / 108766

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.