MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Matexcel GRA-242 Monolayer Graphene on Cu with PMMA Coating
Categories: Carbon

Material Notes: This product is monolayer graphene on Cu substrate with PMMA coating. This pre-coating product can be used to transfer the graphene film by a simple method.

Application: Flexible batteries, Electronics, Aerospace industry, MEMS and NEMS, Microactuators, Conductive coatings, Research

Morphology: Transparent thin layer on copper

Uses: Materials: 1M~2M FeCl3, acetone, deionized water, plastic dropper, tweezers Steps: 1, Prepare two glass culture dishes, each with FeCl3 solution. Hold the sample with a pair of tweezers and place it gently on the surface of FeCl3 solution. The Cu side is in contact with the solution and the surface coated with PMMA is facing up. 2, After 3 minutes of corrosion, clamp a corner of the sample with tweezers and lift the sample vertically from the dish. Pipette the FeCl3 solution with a plastic dropper, rinse three times of the side of the sample that has been corroded(If the first removal is not clean, you can etch for another two minutes after the first corrosion, repeat the rinse once). 3, Gently spread the rinsed sample on the surface of the second culture dish solution. After about 1 hour, the copper was completely etched away. It can be seen that the PMMA film floated on the surface of the solution, and the graphene was on the lower surface of the PMMA film. 4, Picke up the sample from the bottom up using a glass slide and placed in a dish containing deionized water to remove the remaining FeCl3 solution. Repeat three times and using the fresh water for 10 minutes each time(The residue of FeCl3 can be substantially removed after washing three times). 5, Use the substrate you need to pick up the graphene film from the bottom up and put the graphene film in the center of the substrate. Then, keep the sample upright to let the residual water drip. The sample is then placed nearly vertically on the water-absorbing material and dry naturally. 6, After naturally drying, place the sample in 90 centigrade oven or hot stage (110 centigrade) for about 1 hour to let the graphene and the substrate attached closely. 7, After cooled, put the sample in acetone solution to remove PMMA. Repeat three times. Using the fresh acetone each time for 30 minutes (Heating the acetone to 50 degrees can save half time. Heating the acetone also helps to completely remove the pmma, but may cause more graphene damage defects). 8, Remove the sample and let the surface acetone evaporate clean. The sample can be taken for storage. Please put in the oven for 90 centigrade for a half hours before use to remove the attached water molecules.

Key Words: Synonyms: Graphene
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Storage Temperature 20.0 °C
 
Descriptive Properties
Product overviewTransparency: > 97% Coverage: > 97% Number of graphene layers: 1 Thickness (theoretical): 0.345 nm Thickness of Cu substrate: 20-50µm Sheet Resistance: 400±50 Ohms/sq (1cm x1cm)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PMXCK1188 / 299819

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.