Product Description: LL 6202 is a narrow molecular weight butane copolymer designed for applications that require excellent toughness. This resin offers easy processability for applications that require outstanding tear resistance and low warpage. Availability: Latin America, North America and South America Applications: Information provided by ExxonMobil Chemical |