MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Dover Chemical BASE 14L Sulfurized Fatty Compound, Lubricity/Extreme Pressure Additive
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Base 14 L is a sulfurized compound that offers extreme pressure protection and lubricity to straight oil and water dilutable metalworking fluids. Base 14 L formulated fluids exhibit excellent to life and surface finish. Base 14 L contains active sulfur and is thus not recommended for use in materials destined for applications involving yellow metals (copper, bass, or bronze). Base 14 L can be utilized in straight oil machining, drawing and stamping, as well as a soluble oil component. Base 14 L may be stored in an original container or bulk storage tank. Prolonged exposure to 0°F may result in solidification. If the product solidifies, warming to 100-110°F will reconstitute the product. Recommended blending temperatures should not exceed 100-130°F.

Information provided by DoverChem

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.01 g/cc
@Temperature 25.0 °C
Density 8.20 lb/gal
Saybolt Viscosity at 100°F 9000 SUS
Saybolt Viscosity at 210°F 525 SUS
Kinematic Viscosity at 40°C (104°F) 1700 cSt
Kinematic Viscosity at 100°C (212°F) 120 cSt
 
Chemical PropertiesOriginal ValueComments
Total Acid Number 26[mgKOH/g]
 
Thermal PropertiesOriginal ValueComments
Pour Point 70.0 °F
Flash Point >= 177 °CCOC
 
Component Elements PropertiesOriginal ValueComments
Sulfur, S 3.0 %Active
 13 %Total
 
Descriptive Properties
Copper Corrosion3a10% in oil, 3 hrs, 210°F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

WDOVER108 / 217727

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.