MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Teknor Apex Medalist® MD-15155HH Thermoplastic Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Notes: Medalist MD-16155HH is a high performance thermoplastic elastomer (TPE) intended for use in healthcare and medical applications. Medalist MD-16155HH is a medium hardness, medium density, sterilizable grade with good compression set, and high heat resistance that is suitable for injection molding.

Availability: Africa & Middle East; Europe; Asia Pacific; Latin America; North America

Features: Autoclave Sterilizable; Chemical Resistant; Ethylene Oxide Sterilizable; Excellent Elastic Recovery; Good Adhesion; Good Flow; Good Moldability; Good Sterilizability; Halogen Free; Low Compression Set; Medium Density; Medium Hardness; Radiation (Gamma) Resistant

Uses: Gaskets; Hospital Goods; Medical/Healthcare Applications; Membranes; Pharmaceuticals; Plugs; Rubber Replacement; Seal

Agency Ratings: ISO 10993 Part 5; ISO 13485

RoHS Compliance: RoHS Compliant

Form: Pellets

Processing Method: Injection Molding

Preliminary data.

Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.04 g/ccASTM D792
Melt Flow 1.2 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 55
@Time 5.00 sec
ASTM D2240
 58
@Time 1.00 sec
ASTM D2240
Tensile Strength at Break 890 psiDie C, 20 in/min; ASTM D412
Tensile Stress at Strain 350 psi
@Strain 100 %
Die C, 20 in/min; ASTM D412
Elongation at Break 620 %Die C, 20 in/min; ASTM D412
Tear Strength 157 pliDie C, 20 in/min; ASTM D624
Compression Set 13 %
@Temperature 22.8 °C,
Time 79200 sec
Type 1; ASTM D395B
 25 %
@Temperature 70.0 °C,
Time 79200 sec
Type 1; ASTM D395B
 36 %
@Temperature 100 °C,
Time 79200 sec
ASTM D395
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 360 - 420 °F
Middle Barrel Temperature 380 - 440 °F
Front Barrel Temperature 390 - 450 °F
Nozzle Temperature 390 - 450 °F
Melt Temperature 390 - 460 °F
Mold Temperature 70.0 - 100 °F
Back Pressure 25.0 - 100 psi
Cushion 0.150 - 1.00 in
Screw Speed 50 - 100 rpm
 
Descriptive Properties
AppearanceColors Available
 Natural Color
 Opaque

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PTEKNQ0708 / 237199

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.