MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Wacker Silres® BS 280 Silicone Masonry Water Repellent
Categories: Polymer; Thermoset; Silicone

Material Notes: Product description: SILRES® BS 280 is a solvent-free silicone concentrate based on silane/siloxane that is dilutable with organic solvents. Diluted solutions of SILRES® BS 280 are high quality water repellents for impregnating mineral building materials, especially silicate free natural stones like limestone or gypsum. SILRES® BS 280 develops its water repellent effect after application to construction materials as a result of a reaction with atmospheric humidity.

Special features:

  • good penetration into building materials
  • extremely effective with most natural stone
  • good alkali resistance (alkaline mortar joints)
Application: SILRES® BS 280 is particularly recommended for the conservation of monuments and the restoration of natural stone buildings thanks to its all-round effectiveness and excellent alkali resistance. Good results are also achieved when SILRES® BS 280 is used to treat mineral plasters, bricks, sand-lime bricks, aerated concrete and mineral paint.

Information provided by Wacker Chemie AG.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.041 - 1.06 g/ccDIN 12791
Viscosity 7.0 - 9.0 cPdynamic; DIN 51562
 
Thermal PropertiesOriginal ValueComments
Flash Point 49.0 °C
Ignition Temperature 260 °CDIN 51794
 
Descriptive Properties
Appearanceclear to hazy, colorless
Content (%)100Silane/Siloxane

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PWACK9544 / 205073

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.