MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Shin-Etsu Silicones KE-2090-20A/B Self-adhesive LIMS Silicone
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE); Silicone; Silicone Rubber; Liquid Silicone Rubber (LSR)

Material Notes: ShinEtsu KE209020 is a selective self-adhesive liquid injection molding silicone. It is supplied as two components which are mixed in a 1:1 ratio to ensure easy and accurate blending. The viscosity of KE209020 is low enough to allow easy pumping through most injection molding systems

Information Provided by Shin-Etsu Silicones of America, Inc.

Key Words: liquid injection molding silicone, LSR
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.07 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 21
Tensile Strength at Break 1050 psi
Elongation at Break 970 %
Tear Strength 35.0 pliDie B
 
Processing PropertiesOriginal ValueComments
Cure Time 15.0 min
 
Descriptive Properties
Cure TypePress Cure

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Shin-Etsu Silicones LIMS™ KE2090-40AB Elastomer
Covestro Makrolon® 2858 Polycarbonate, Injection Grade
Lotte Advanced Materials Infino® PCA-NH1015V Flame Retardant
CHT Group QSil 213 Transparent, Liquid Silicone Rubber
Dow C6-530 LIQUID SILICONE RUBBER KIT

PSHIN218 / 177729

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.