MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Bostik GreenFusion2™ Flooring Adhesive
Categories: Polymer; Adhesive; Renewable/Recycled Polymer; Thermoset

Material Notes: Description: Bostik GreenFusion2™ is an ultra premium, high strength, solvent free, two-component, urethane adhesive. It is specifically formulated for the installation of most rubber, homogenous PVC, solid vinyl and artificial grass carpet in the most demanding environments where extra heavy traffic, rolling loads or extreme climatic conditions may exist or might occur. GreenFusion2™ is a 0-VOC formulation as calculated per SCAQMD Rule 1168 that contains 27% rapidly renewable material. Once cured, this adhesive is not adversely affected by exposure to moisture or water; its superior properties provide a tenacious bond to a variety of surfaces either indoors or outdoors. GreenFusion2™ has been formulated to exhibit a unique combination of application properties including excellent trowelability, low odor and easy clean up. GreenFusion2™ may be used over all properly prepared substrates common to resilient flooring installations including; concrete, asphalt, plywood, cementitious-based patch/underlayment, terrazzo, and radiant heat systems. GreenFusion2™ comes with Bostik’s BLOCKADER antimicrobial protection, which inhibits the growth of bacteria, mold, or mildew on the surface of the dried adhesive; the dried adhesive resists stains caused by mold or mildew..

Key Features:

  • Interior or harsh exterior uses
  • 27% rapidly renewable material

Information provided by Bostik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 13.2 lb/gal
Solids Content 100 %
Volatile Organic Compounds (VOC) Content 0.00 g/l
pH 5.0 - 12
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 92
Hardness, Shore D 35
 
Thermal PropertiesOriginal ValueComments
Flash Point >= 300 °F
 
Processing PropertiesOriginal ValueComments
Working Life 30.0 - 45.0 min
 
Descriptive Properties
ColorBeige
Recycled Content27%

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Arkema Pebax® Rnew® 55R53 SP 01 Polyether Block Amide (PEBA)
Telles Mirel™ I6001 Biobased Polymeric Modifier
FKuR Kunststoff Terralene® LL 1303 Biobased Polyethylene
Geon® Performance Solutions Vinyl Wire & Cable W1201 Polyvinyl Chloride, Flexible
BASF Ecoflex® F BX 7011 Biodegradable Plastic

PBOSTK042 / 191578

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.