MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Extreme Materials from MCAM
Visit Mitsubishi Chemical Advanced Materials for Extreme Materials - high performance plastic machining stock engineered to replace metals such as nickel alloys or stainless steel.

(Viewing data as-entered. Click here to return)
ATI Allegheny Ludlum AL 400™ Nickel-Base Alloy, Annealed Plate, Sheet, and Strip, UNS N04400
Categories: Metal; Nonferrous Metal; Nickel Alloy; Superalloy

Material Notes: Moderately to faintly magnetic at room temperature. Allegheny Ludlum AL 400 alloy is a ductile nickel-copper alloy with resistance to a variety of corrosive conditions. The alloy is most frequently applied in a range of environments ranging from mildly oxidizing through neutral and to moderately reducing conditions. An additional application area of the material is in marine environments and other nonoxidizing chloride solutions. Specific uses include chemical or refining process equipment, pumps, valves, and fittings.

The alloy has a long history of use as a corrosion resistant material, dating back to the early twentieth century when it was developed as an attempt to use a high copper content nickel ore. The nickel and copper contents of the ore were in the approximate ratio which is now formally specified for the alloy.

As with commercially pure nickel, the AL 400 alloy is low in strength in the annealed condition. For this reason, a variety of tempers are used which have the effect of increasing the strength level of the material.

Information provided by Allegheny Ludlum

Key Words: DIN 2.4360; ASTM B-127; ASME SB-127; AMS 4544
Vendors: Visit metalmen for your metals needs. Products include special chemistry, tight tolerances, custom tempers, odd dimensions/forms, and small quantities. Phone 1-800-767-9494.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 8.83 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell B 70Typical Annealed
Tensile Strength, Ultimate 520 MPaTypical
Tensile Strength, Yield 240 MPaTypical
Elongation at Break 45 %Typical in 2"
Modulus of Elasticity 180 GPaTypical
Charpy Impact 135 - 325 J
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000510 ohm-cm
 
Thermal PropertiesOriginal ValueComments
CTE, linear 13.9 µm/m-°C
@Temperature 20.0 - 93.0 °C
 15.8 µm/m-°C
@Temperature 20.0 - 315 °C
 16.4 µm/m-°C
@Temperature 20.0 - 538 °C
Specific Heat Capacity 0.430 J/g-°C
Thermal Conductivity 24.1 W/m-K
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al 0.020 %
Carbon, C 0.10 %
Copper, Cu 32 %
Iron, Fe 1.0 %
Manganese, Mn 0.50 %
Nickel, Ni 66 %as balance; includes Co
Phosphorus, P 0.0050 %
Silicon, Si 0.25 %
Sulfur, S 0.0050 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
304 Stainless Steel (UNS S30400); Annealed Plate
316 Stainless Steel, annealed plate
Special Metals MONEL® Alloy 400
310 Stainless Steel, annealed sheet
ATI Allegheny Ludlum AL 400™ Nickel-Base Alloy, Hot Rolled Plate, UNS N04400

NLN40A / 18014

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.