MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
PSM Industries Pacific Sintered Metals BZ-111-U Yellow Brass Powdered Metal (MPIF CZP-2000-11)
Categories: Metal; Nonferrous Metal; Copper Alloy; Brass

Material Notes: Applications: 80-20 leaded brass for structural and hardware components.

Equivalent MPIF Specification: CZP-2000-11

All information provided by Pacific Sintered Metals.

Key Words: PM
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.60 - 7.80 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell H 70
Tensile Strength, Ultimate 23000 psi
Tensile Strength, Yield 13500 psi
Elongation at Break 12 %
Flexural Strength 50000 psiTransverse Rupture
Charpy Impact, Unnotched 28.0 ft-lb
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000069 ohm-cm
 
Descriptive Properties
Electrical Conductivity (% IACS)25

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Uninhibited Naval brass, UNS C46400, O60 Temper 6 mm flat products
Architectural Bronze, UNS C38000
Antimonial Naval brass, UNS C46600, O61 Temper tubing
Antimonial Naval brass, UNS C46600, O60 Temper 6 mm flat products
Antimonial Naval brass, UNS C46600, O50 Temper 1 mm flat products

NPACIF035 / 86193

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.