MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Hexcel® HexPly® M48 180°C/356°F Curing Epoxy Matrix, M48/42%/48370/1000  (discontinued **)
Categories: Polymer; Thermoset; Epoxy; Epoxy Cure Resin

Material Notes: Fiber: HR 12K, 2x2 Twill, 370 g/m2

Information provided by HexCel

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.28 g/ccResin
 1.53 g/ccNominal Laminate
 1.78 g/ccFiber
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 1022 MPa
@Temperature 23.0 °C
prEN2561 Type B
Tensile Modulus 58.0 GPa
@Temperature 23.0 °C
prEN2561 Type B
Compressive Yield Strength 200 MPa
@Temperature 23.0 °C
Compression After Impact @ 6.7 J/mm; AITM 1.0010
 765 MPa
@Temperature 23.0 °C
prEN2580 Type B
Compressive Modulus 50.0 GPa
@Temperature 23.0 °C
prEN2580 Type B
Shear Modulus 4.60 GPa
@Temperature 23.0 °C
In-Plane; prEN6032
Shear Strength 48.4 MPa
@Temperature 23.0 °C
ILSS; prEN2563
 77.0 MPa
@Temperature 23.0 °C
In-Plane; prEN6032
 
Thermal PropertiesOriginal ValueComments
Glass Transition Temp, Tg 201 °COnset
 218 °CPeak
 
Processing PropertiesOriginal ValueComments
Shelf Life 12.0 Month
@Temperature -18.0 °C
 
Descriptive Properties
Cured Thickness per Ply (cm)0.0417
Fiber Volume (%)49.8
Tack Life (days)15

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Solvay MTM® 248S Epoxy
Solvay MTM® 71 Epoxy Matrix Resin
Solvay LTM® 26EL Epoxy with T300 Woven Carbon Fiber Laminate
Solvay CYCOM® 890 RTM Resin - Woven Carbon Fabric Composite
Park Aerospace Nelcote® E-765 Epoxy Prepreg, T700 12K 2x2 Twill Reinforced

PHEXC192 / 98663

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.