MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Precision Polymer Engineering Perlast® G60H Perfluoroelastomer
Categories: Polymer; Thermoset; Fluoropolymer, TS; Thermoset Fluoroelastomer; Rubber or Thermoset Elastomer (TSE)

Material Notes: Special, pure white compound with excellent high temperature properties and wide chemical resistance. Extremely low outgassing properties.

Applications: For use in applications which require exposure to temperatures in excess of 260°C (500°F) and shorter term to 310°C (590°F). Recommended for use in the semiconductor industry. Do not use any Perlast ® grade with molten alkali metals.

Key Words: Rubbers
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 58°IRHD, -2 change after 72 hours @ 260°C; ASTM D1415
 60°IRHD; ASTM D1415
Tensile Strength, Yield 13.0 MPaASTM D412
 14.3 MPa10% change after 72 hours @ 260°C; ASTM D412
Elongation at Break 237.5 %-5% change after 72 hours @ 260°C; ASTM D412
 250 %ASTM D412
100% Modulus 0.00720 GPa
@Strain 100 %
-10% change after 72 hours @ 260°C; ASTM D412
 0.00800 GPa
@Strain 100 %
ASTM D412
Compression Set 19 %
@Temperature 200 °C,
Time 86400 sec
ASTM D395
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 310 °C
Minimum Service Temperature, Air -15.0 °C
Flash Point >= 400 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Precision Polymer Engineering Perlast® G71H Perfluoroelastomer
Precision Polymer Engineering Perlast® G70T Perfluoroelastomer
Precision Polymer Engineering Perlast® G70R Red Perfluoroelastomer
Precision Polymer Engineering Perlast® G70K Perfluoroelastomer
Precision Polymer Engineering Perlast® G70H Perfluoroelastomer

PPRECI002 / 57726

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.