MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Syensqo (Solvay Specialty Polymers) Amodel® A-4133 HH PPA, 35% glass fiber
Categories: Polymer; Thermoplastic; Polyphthalamide (PPA); Polyphthalamide (PPA), 40% Glass Fiber Reinforced

Material Notes: Amodel® A-4133 HH BK is a 35% glass fiber reinforced heat stabilized grade of polyphthalamide (PPA) that has been designed to provide outstanding property retention to thermal oxidative degradation at temperatures of 230°C. Other features are fast cycling and hot water moldability. This product is particularly suitable to air induction applications within downsized automotive engines such as air induction charge air cooling and exhaust gas recirculation.

This grade features high heat deflection temperature, high flexural modulus and high tensile strength, as well as excellent creep resistance and low moisture absorption.

- Black: A-4133 HH BK 311

Applications: Automotive Applications; Automotive Electronics; Connectors; Consumer Applications; Housings; Industrial Applications; Machine/Mechanical Parts; Metal Replacement

Features: Chemical Resistant; Creep Resistant; Good Dimensional Stability; Good Stiffness; Heat Stabilized; High Heat Resistance; High Strength; Hot Water Moldability; Laser Weldable; Low Moisture Absorption

Injection notes: Injection Rate: 3 to 4 in/sec
Holding Pressure: 50% of injection pressure
Storage:
- Amodel® compounds are shipped in moisture-resistant packages at moisture levels according to specifications. Sealed, undamaged bags should be preferably stored in a dry room at a maximum temperature of 50°C (122°F) and should be protected from possible damage. If only a portion of a package is used, the remaining material should be transferred into a sealable container. It is recommended that Amodel® resins be dried prior to molding following the recommendations found in this datasheet and/or in the Amodel® processing guide.
Proper Ventilation:
- It is strongly recommended that the processing site be correctly ventilated during molding. The ventilation should be placed directly above the injection nozzle to prevent exposure to fumes and gases that may be generated.
- In the event of a barrel purge where a large melt patty may be generated, it is often advisable to draw the purge patty into a bucket of water to reduce fumes.
Hot Runners:
- Solvay does not encourage the use of hot runner technology with this product. For further clarification on hot runners, please contact your Solvay Specialty Polymers Technical Marketing representative.

Information provided by Solvay Specialty Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.49 g/ccMethod A; ISO 1183
Water Absorption 0.50 %
@Time 86400 sec
ASTM D570
Linear Mold Shrinkage, Flow 0.0030 cm/cmASTM D955
Linear Mold Shrinkage, Transverse 0.010 cm/cmASTM D955
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 41.0 MPa
@Temperature 250 °C
ISO 527-2
 49.0 MPa
@Temperature 200 °C
ISO 527-2
 56.0 MPa
@Temperature 200 °C
ISO 527-2
 64.0 MPa
@Temperature 180 °C
ISO 527-2
 92.0 MPa
@Temperature 120 °C
ISO 527-2
 214 MPa
@Temperature 23.0 °C
ISO 527-2
 245 MPa
@Temperature -40.0 °C
ISO 527-2
Elongation at Break 2.1 %ISO 527-2
Tensile Modulus 12600 MPaISO 527-2
Flexural Strength 279 MPaISO 178
Flexural Modulus 11100 MPaISO 178
Compressive Strength 161 MPaASTM D695
Poissons Ratio 0.39ASTM E132
Shear Strength 88.0 MPaASTM D732
Izod Impact, Notched (ISO) 9.00 kJ/m²Type 1, Notch A; ISO 180
Izod Impact, Unnotched (ISO) 52.0 kJ/m²Type 1; ISO 180
Charpy Impact Unnotched 60.0 kJ/m²Type 1, Edgewise; ISO 179
Charpy Impact, Notched 8.00 kJ/m²Type 1, Edgewise, Notch A; ISO 179
 
Thermal PropertiesOriginal ValueComments
Melting Point 327 °CISO 11357-3
Deflection Temperature at 1.8 MPa (264 psi) 285 °CUnannealed; ISO 75-2/A
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 318 - 324 °C
Middle Barrel Temperature 318 - 324 °C
Front Barrel Temperature 327 - 332 °C
Melt Temperature 330 - 335 °CInjection
Mold Temperature 66.0 - 93.0 °C
Drying Temperature 120 °C
@Time 14400 sec
Moisture Content <= 0.045 %Injection
 
Descriptive Properties
AdditiveHeat Stabilizer
AvailabilityEurope
 North America
ColorBlack
FormsPellets
ProcessingWater-Heated Mold Injection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSOL8Y4053 / 279853

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.