MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Go Yen Chemical GGK-1300 Wear Resistant Coupling Agent
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Offer various synthetic resin good impact strength and rubbing strength

Advantages:

  • offer various synthetic resin good impact strength and rubbing strength.
  • GGK-1300 has low surface tension and viscosity Reduction applied in PU,EPOXY,UP etc. resin related products, enhancing good wear resistance
  • GGK-1300 has good processing compatibility with resin
  • give various plastic excellent tinting strength and trafficability
  • give product good slip velocity and lubricity.
  • give constructional material, board and resin high wear resistance It applied in outdoor synthetic products and has good weather resistance and antioxidant ability.
  • the suggested adding volume is approx 2%~7%. User can adjust it according different formula and need of client
Applications:
  • various thermal plastic elamoster(TPU, TPE, SBS, SEBS..)
  • plastic: PVC, PP, PE, PS constructional board and floorboard.
  • various rubber industry(CR, CSM, NR, SBR, SIR….etc.)
  • synthetic PU leather, PVC.NYLON related products (special synthetic leather, various sports ball synthetic leather, industry brake pad, sofa leather, massage chair leather etc.)
  • enhance wear resistance of unsaturated resin (UP RESIN). It’s applied in BMC, SMC, FRP…etc manufacturing process to enhance wear resistance of board.
  • polycarbonate, nylon, polyacetal, polysulfide, polyester product
  • resin coating and various wear resistance of surface treatment agent
  • other special application

Information provided by Go Yen Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Particle Size <= 1.0 µm0.5
 1.0 µmAverage particle size
 <= 2.0 µm0.733
 <= 3.0 µm0.9
 
Processing PropertiesOriginal ValueComments
Moisture Content <= 1.0 %
 
Descriptive Properties
AppearanceWhite powder

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PGOYEN321 / 266629

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.