MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Celanese Celstran® PA66-GF40-02-US Nylon 66, 40% Glass Reinforced
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 40% Glass Fiber Filled

Material Notes: 40% Long glass fiber reinforced, heat stabilized, Nylon 6/6

Information provided by Celanese

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.45 g/ccASTM D792
Density 1.45 g/ccISO 1183
Linear Mold Shrinkage, Flow 0.0010 - 0.0020 cm/cmASTM D955
Linear Mold Shrinkage, Transverse 0.0020 - 0.0030 cm/cmASTM D955
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 215 MPa5mm/min; ISO 527-2/1A
 36700 psiASTM D638
 19400 psi
@Temperature 121 °C
ASTM D638
 39100 psi
@Temperature -40.0 °C
ASTM D638
Tensile Strength 120 MPa
@Temperature 80.0 °C
ISO 527-1, -2
Elongation at Break 2.0 %5mm/min; ISO 527-2/1A
 2.3 %ASTM D638
 2.2 %
@Temperature 4.44 °C
ASTM D638
 2.5 %
@Temperature 121 °C
ASTM D638
 2.9 %
@Temperature 80.0 °C
ISO 527-1, -2
Tensile Modulus 13300 MPa50mm/min; ISO 527-2/1A
 2.06e+6 psiASTM D638
 7500 MPa
@Temperature 80.0 °C
ISO 527-1, -2
 1.06e+6 psi
@Temperature 121 °C
ASTM D638
 2.10e+6 psi
@Temperature -40.0 °C
ASTM D638
Flexural Strength 355 MPaISO 178
 52000 psiASTM D790
 210 MPa
@Temperature 80.0 °C
ISO 178
 26300 psi
@Temperature 121 °C
ASTM D790
 56300 psi
@Temperature -40.0 °C
ASTM D790
Flexural Modulus 13500 MPaISO 178
 1.78e+6 psiASTM D790
 6800 MPa
@Temperature 80.0 °C
ISO 178
 940000 psi
@Temperature 121 °C
ASTM D790
 1.805e+6 psi
@Temperature -40.0 °C
ASTM D790
Izod Impact, Notched 6.90 ft-lb/inASTM D256
 7.40 ft-lb/in
@Temperature -40.0 °C
ASTM D256
 8.70 ft-lb/in
@Temperature 149 °C
ASTM D256
Izod Impact, Notched (ISO) 43.0 kJ/m²
@Temperature -30.0 °C
ISO 180/1U
 47.0 kJ/m²
@Temperature 23.0 °C
ISO 180/1U
Charpy Impact Unnotched 95.0 kJ/m²ISO 179/1eU
 46.0 kJ/m²
@Temperature -30.0 °C
ISO 179/1eU
Charpy Impact, Notched 35.0 kJ/m²ISO 179/1eA
 26.0 kJ/m²
@Temperature -30.0 °C
ISO 179/1eA
Puncture Energy 17.8 JISO 6603-2
 
Thermal PropertiesOriginal ValueComments
Melting Point 261 °C10°C/min; ISO 11357-1,-2,-3
Deflection Temperature at 1.8 MPa (264 psi) 255 °CISO 75-1, -2
 490 °FASTM D648
Deflection Temperature at 8.0 MPa 240 °CISO 75-1, -2
 
Processing PropertiesOriginal ValueComments
Processing Temperature 80.0 - 100 °Ccavity
Feed Temperature 20.0 - 50.0 °C
Zone 1 285 - 295 °C
Zone 2 290 - 300 °C
Zone 3 300 - 310 °C
Zone 4 300 - 315 °C
Die Temperature 300 - 315 °C
Melt Temperature 305 °CISO 294
 300 - 315 °C
Mold Temperature 90.0 °CISO 294
Injection Velocity 80.0 mm/secISO 294
Drying Temperature 70.0 - 80.0 °C
Dry Time 2.00 - 4.00 hour
Moisture Content <= 0.18 %
Hold Pressure 83.0 MPaISO 294
 
Descriptive Properties
Injection moldingYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Celanese Celstran® PA66-GF40-01 Nylon 66, 40% Glass Reinforced
Celanese Celstran® PA66-CF40-02 AF3004 Natural Nylon 66, 40% LCF
Celanese Celstran® PA6-GF40-01 Nylon 6, 40% Glass Reinforced
Envalior Akulon® Diablo HT-HG6 (K-X07031) PA66+PA6-GF30, Dry, 30% Glass Filled, Heat Stabilized
Celanese VECTRA A950 LCP, Unfilled

PHCQ166 / 178621

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.