MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Borealis BorSafe™ ME3440-W MDPE
Categories: Polymer; Thermoplastic; Polyethylene (PE); Medium Density (MDPE)

Material Notes: BorSafe ME3440-W is a bimodal polyethylene compound produced by the advanced Borstar technology. The product is a medium-density polyethylene compound in pellet form and contains a combination of stabilizers and carbon black to ensure a reliable long-term stability and UV-resistance. BorSafe ME3440-W is classified as an MRS 8.0 material (PE80).

Applications:

  • Cable protection pipes
  • Irrigation pipes
  • Drinking water
  • Relining
  • Gas distribution
  • Sheets and profiles
  • Industrial applications
BorSafe ME3440-W is recommended for pressure pipe systems in the application fields above.

Specifications: BorSafe ME3440-W is expected to meet the applicable requirements included in the below mentioned standards provided it is processed using sound material handling and processing practices as well as appropriate testing procedures. EN 12201; ISO 4427; EN 1555; ISO 4437; EN ISO 15494

BorSafe ME3440-W provides an improved performance level in terms of drinking water related requirements such as migration limits. The sensoric properties like taste & odor are regularly monitored for the compound to ensure a high constant level of quality. The material shows excellent mechanical toughness and crack resistance also at lower temperatures. Thanks to the molecular structure, it offers outstanding extrudability and good melt strength, supporting a problem-free extrusion process to tight tolerances.

Information provided by Borealis AG

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.954 g/ccISO 1183-1
Oxidative Induction Time (OIT) >= 20.0 min
@Temperature 210 °C
ISO 11357-6
Carbon Black Loading 2.00 - 2.50 %ISO 6964
 <= 3.00 %dispersion; ISO 18553
Melt Flow 0.800 g/10 min
@Load 5.00 kg,
Temperature 190 °C
ISO 1133-1
Storage Temperature <= 50.0 °C
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 20.0 MPa50 mm/min; ISO 527-2
Elongation at Break >= 600 %50 mm/min; ISO 527-2
Tensile Modulus 800 MPa1 mm/min; ISO 527-2
 
Processing PropertiesOriginal ValueComments
Processing Temperature 180 - 210 °CCylinder
Die Temperature 200 - 210 °C
Melt Temperature 200 - 220 °C
Head Temperature 200 - 210 °C
Shelf Life 24.0 Month
 
Descriptive Properties
Resistance to rapid crack propagation>1 barS4 test, Pc at 0°C, Test pipe 250mm, SDR11; ISO 13477
Resistance to slow crack growth>2000 h8 bar 80 °C, ISO 13479

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PBORE9669 / 323026

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.